1.Technical tsis ntawm alumina ceramic muab tub lim

2. Cov khoom piav qhia
Lub ntsiab raw khoom rau alumina ceramic muab tub lim yog high-purity aluminium oxide hmoov. Thaum lub sij hawm ntau lawm, yuav tsum tau ntxiv ib co additives thiab binders. Tom qab kev tshuaj ntsuam, ziab thiab lwm yam kev kho mob ua ntej, lav qhov loj me me yog qhov sib xws thiab cov ntsiab lus noo noo yog nruab nrab. Txais siv dov txoj kev thiab isostatic nias, cov pob tsim tau qhuav ntawm qhov kub ntawm 100-150 degree , thiab thaum kawg sintered ntawm qhov kub kub ntawm 1500-1700 degree
Aluminium oxide ceramic muab tub lim tau muab faib ua peb tus qauv: TYPE92, TYPE95, thiab TYPE99 raws li cov ntsiab lus sib txawv ntawm txhuas oxide, uas tsim nyog rau cov neeg siv khoom sib txawv. Cov khoom muaj siab purity, ob peb impurities, siab ceev, siab hardness, zoo hnav tsis kam, muaj zog acid thiab alkali corrosion kuj, thiab tau dav siv nyob rau hauv petrochemical nroj tsuag, tshuaj fiber ntau nroj tsuag, ethylene nroj tsuag, cracking khoom, catalytic khoom, thiab lwm yam. Nws txoj haujlwm yog txhawm rau nce cov ntsiab lus ntawm cov roj thiab kua, txhawb nqa thiab tiv thaiv cov catalysts uas tsis muaj zog
3. Khoom specifications
Φ 3mm, Φ 6mm, Φ 8mm, Φ 9mm, Φ 10mm, Φ 13mm, Φ 16mm, Φ 19mm, Φ 25mm, Φ 30mm, Φ 38mm, Φ 50mm, Φ 6mm
4. Cov yam ntxwv tseem ceeb ntawm cov khoom
1) High purity, tsawg impurities, Fe2O3 Tsawg dua los yog sib npaug rau 0.2%
2) High ceev, siab hardness, muaj zog hnav tsis kam, Mohs hardness Ntau dua los yog sib npaug rau 9
3) Muaj zog acid thiab alkali corrosion kuj, tshwj tsis yog rau hydrofluoric acid, resistant rau ntau yam organic thiab inorganic acids corrosion
4) Zoo thermal shock stability, txo los ntawm 1200 degree mus rau 600 degree, tsis muaj kab nrib pleb tom qab 10 cycles
5) Zoo ntim stability, 1400 degree * 12h, shrinkage tus nqi Tsawg dua los yog sib npaug rau 0.2%
5. Daim ntawv thov khoom
Cov khoom siv dav siv hauv cov cuab yeej tawg, cov khoom siv catalytic, thiab lwm yam khoom siv catalytic hauv cov nroj tsuag petrochemical thiab ethylene. Nws txoj haujlwm yog txhawm rau nce cov ntsiab lus ntawm cov pa roj thiab cov kua dej, txhawb nqa thiab tiv thaiv cov catalysts
6. Cov neeg siv khoom ua tau zoo

Koj puas xav nrhiav tus kws tshaj lij ntawm alumina ceramic muab tub lim?
Koj puas xav nrhiav tus neeg muag khoom ruaj khov thiab ntseeg tau?
Tom qab ntawd thov hu rau peb
Hu rau kuv:
Email: wp@cnjingganrefractory.com/sdwenping@163.com
TEL: 86-0533-4188518 / Fax: 86-0533-4188518
Rose: +86-13275332819(wechat/whatsapp tus xov tooj)
Cim npe nrov: alumina ceramic muab tub lim, Tuam Tshoj, tuam ntxhab, lwm tus muag khoom, Hoobkas, siv, khoom