Unshaped refractory khoom yog cov khoom siv refractory tsim los ntawm cov khoom siv refractory aggregate nrog qee qhov me me faib, hmoov, khi, thiab cov khoom sib xyaw, tseem hu ua dispersed refractory khoom. Siv rau hauv ob sab phlu ntawm cov khoom siv thermal, ncaj qha ci yam tsis tau mus los ntawm kev tua hluav taws. Piv nrog rau cov hluav taws kub-resistant bricks, nws muaj cov yam ntxwv ntawm cov txheej txheem yooj yim (tshem tawm cov txheej txheem tua hluav taws), txuag hluav taws xob, tus nqi qis, thiab kev siv tshuab yooj yim.
Muaj peb yam rau kev ua tau zoo ntawm cov khoom Asian refractory:
(1) Mechanical zog. Xws li compressive zog thiab flexural zog.
(2) Cov khoom siv tshuaj. Xws li slag kuj thiab cov tshuaj tiv thaiv nrog cov cua tswj tau.
(3) Lub cev ua haujlwm. Xws li qhov ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntom ntim cov tshuab ua kom zoo nkauj zoo nkauj thermal conductivity Raws li lub hom phiaj ntawm cov ntaub ntawv refractory, pib los ntawm kev sib piv ntawm ntau yam uas yuav tsum tau muaj, xaiv ntau hom refractory cov ntaub ntawv, thiab thaum kawg paub tseeb tias lawv raws li kev nqis peev thiab nyiaj txiag cov txiaj ntsig.
Kev ua haujlwm ntawm cov khoom siv amorphous refractory yog hais txog kev ua haujlwm zoo uas ntsuas qhov nyuaj ntawm kev tsim kho cov khoom siv amorphous refractory. Kev ua haujlwm tau zoo, uas txhais tau hais tias cov khoom siv amorphous refractory tuaj yeem sib xyaw, thauj, nchuav, sib sau ua ke, txau thiab lwm yam kev tsim kho hauv kev ua haujlwm txuag nyiaj, ua tiav kev ruaj ntseg thiab ceev thaum kawg tsim.
Qhov zoo ntawm kev ua haujlwm ncaj qha cuam tshuam rau kev ua haujlwm zoo thiab kev tsim kho, thiab nws feem ntau ntseeg tias kev ua haujlwm muaj xws li kev ua tau zoo ntawm plaub yam khoom: fluidity, plasticity, stability, thiab compactness ntawm qhov sib tov.
1. Flowability: Nws nyob ntawm qhov kev faib ua feem ntawm cov khoom-kua theem nyob rau hauv qhov sib tov, thiab feem ntau nce nrog cov ntsiab lus ntawm cov dej, uas ua rau muaj kev nce hauv flowability.
2. Plasticity: hais txog lub peev xwm los tsim cov yas deformation yam tsis muaj "nkig tawg" nyob rau hauv ib qho kev quab yuam sab nraud, uas cuam tshuam rau cov dej cement piv thiab cov ntsiab lus ntawm cov cement slurry los yog binder.
3. Stability: yog hais txog qhov kev nyuab siab shear generated los ntawm lub ntiajteb txawj nqus ntawm cov aggregate nyob rau hauv cov sib tov, uas tsis pub tshaj qhov yield stress ntawm "kua theem". Qhov sib tov ruaj khov ua rau nws nyuaj rau cov khoom sib xyaw ua ke rau txheej thiab los ntshav raws li qhov loj me.
4. Tightness: yog hais txog lub peev xwm ntawm kev sib tov kom kov yeej cov kev tiv thaiv sab hauv thiab saum npoo thiab ua tiav compaction thaum vibration lossis compaction.
Plaub qhov kev xav tau rau kev ua haujlwm ntawm amorphous refractory cov ntaub ntawv hais los saum toj no tuaj yeem cuam tshuam nrog ib leeg hauv ntau qhov xwm txheej. Kev ruaj ntseg yuav tsum tau sib tov kom muaj kev sib txuam siab kom txo tau cov dab dej thiab los ntshav ntawm cov coarse aggregates, thaum compactness xav tau cov sib tov kom tsis muaj cohesion thiab kev sib txhuam sab hauv kom compaction yooj yim dua. Yog li ntawd, kev ua haujlwm ntawm qhov sib tov yuav tsum tau txiav txim siab raws li qhov xav tau ntawm cov sijhawm sib txawv.