Ceramic rollers tau muab faib ua siab aluminium ceramic rollers, siab aluminium silicon carbide ceramic rollers, thiab silicon carbide ceramic rollers. Lawv yog cov khoom siv sib kis tau tsim tshwj xeeb rau cov menyuam cov kiln, nrog kev ua haujlwm kub siab tshaj 1300 degree. High ntsuab ceramic rollers muaj ntau qhov ntau thiab tsawg, nrog rau Al2O3 cov ntsiab lus ntau dua 70 feem pua, thiab feem ntau siv rau hauv thaj chaw tua hluav taws. High aluminium silicon carbide rollers feem ntau siv rau hauv txoj siv txias ntawm cov kilns, nrog kev ua haujlwm zoo rau kev ua kom txias thiab cua sov, lub neej ua haujlwm ntev, thiab kev tiv thaiv kev tawg.
Ceramic rollers yog cov khoom siv tshwj xeeb rau kev tsim cov vuas luaj ceramic. Lawv tsis khoov lossis deform thaum siv, muaj qhov zoo compressive thiab khoov lub zog, thermal shock stability, thiab hnav tsis kam.