Bending zog ntawm Refractory

Feb 01, 2023

Bending zog yog hais txog qhov siab tshaj plaws dabtsi yog khoov kev nyuaj siab uas tus qauv refractory tuaj yeem dais ntawm peb-point dabtsi yog khoov ntaus ntawv, tseem hu ua dabtsi yog khoov zog. Lub zog dabtsi yog khoov ntawm cov ntaub ntawv refractory yog muab faib ua qhov kub thiab txias dabtsi yog khoov lub zog thiab kub kub dabtsi yog khoov zog. Feem ntau, cov khoom uas muaj siab compressive zog ntawm ib txwm kub muaj siab flexural zog ntawm ib txwm kub. Cov khoom uas muaj lub zog flexural siab ntawm qhov kub thiab txias muaj qhov ua haujlwm zoo rau kev cuam tshuam, hnav thiab yaig ntawm cov ntaub ntawv thiab cov kua slag nyob rau hauv qhov kub thiab txias ntawm kev siv. Qhov feem ntau siv yog Mpa, N / mm2.

 

 

 

 

 

 

 

Hu rau kuv:

Email: wp@cnjingganrefractory.com/sdwenping@163.com

TEL: 86-0533-4188518 / Fax: 86-0533-4188518

Rose: ntxiv rau 86-13275332819(wechat/whatsapp tooj)