Lub plawv dub yog ib qho yooj yim tshwm sim hauv txhuas cib ntau lawm. Cov ua thiab tej yam kev mob ntawm lub plawv dub yog raws li nram no

Lub ntsiab impurity oxides hauv siab alumina cib yog Fe2O3 thiab TiO2, uas yog cov xwm txheej rau kev tsim lub siab dub. Txawm li cas los xij, thaum hlau thiab titanium oxides nyob ib leeg, lawv muaj qhov sib txawv ntawm cov xim ntawm cov khoom. Thaum titanium ions nyob ib leeg, cov xim tsis tseem ceeb, thiab cov khoom zoo li xiav me ntsis, thaum thaum hlau ions nyob ib leeg, cov khoom tshwm xim av. Txawm li cas los xij, kev sib koom ua ke ntawm hlau thiab titanium tuaj yeem ua kom cov xim ntawm cov khoom lag luam txawm tias nyob hauv qhov chaw oxidizing. Nyob rau hauv ib qho kev txo qis, kev sib koom ua ke ntawm hlau thiab titanium ions ib leeg tuaj yeem tsim cov chaw dub hauv cov xim ntawm cov khoom.

Txoj hauv kev kom tsis txhob dub chaw nyob hauv siab alumina cib:

1) Lub siab titanium bauxite raw khoom yuav raug tshem tawm cov hlau nplaum muaj zog kom txo qis kev sib koom ua ke ntawm titanium thiab hlau ions

2) Hloov cov txheej txheem kev them nyiaj ntawm lub siab alumina cib, txoj kev hluav taws kub yog loj thiab du, thiab cov xuab zeb cushion ntawm cib yog tag nrho.

3) Ua kom cov cua kub kom tsim tau cov pa oxygen enriched

4) Thaum lub sij hawm txias, txias qeeb kom tsis txhob decolorization vim re oxidation ntawm hlau thiab titanium ions