Kev tiv thaiv ib puag ncig magnesia alumina carbon cib tau txhim kho hauv kev xaiv cov khoom thiab txheej txheem tsim khoom. Yog li ntawd, kev tiv thaiv ib puag ncig magnesia alumina carbon cib txawv ntawm cov tsoos magnesia alumina carbon cib
1. Cov khoom siv xaiv: cov khoom xaiv ntawm cov khoom muaj ntau dua 97% MgO fused magnesia, ntau dua 98% Al2O3 fused corundum, ib puag ncig tiv thaiv cob thiab antioxidant micro hmoov
2. Kev tsim: nws yog tsim los ntawm 500t hydraulic xovxwm lossis 1000t txhuam xovxwm kom ntseeg tau tias qhov tseeb ntawm cov cib ntom ntom ntom, qhov ntxeem tau thiab qhov loj me
3. Kub ci: qhov ntsuas kub ntawm cov khoom yog 300 ± 10 ℃, Yog li ntawd, qhov ceev ntawm ib puag ncig-phooj ywg magnesium aluminium carbon cib yog qhov loj, uas yog 3.10-3.15g/cm3, porosity tsawg, uas yog kwv yees li 3.2 %, thiab lub zog nrawm yog siab, uas ntau dua lossis sib npaug rau 60MPa. Yog li ntawd, nws muaj cov tshuaj tiv thaiv corrosion zoo dua qub thiab ua haujlwm ntev dua