Cov menyuam lub qhov cub tseem hu ua cov menyuam hauv qab ncu. Nws yog tsuas yog siv nyob rau hauv kev tsim cov ceramic tsev cov ntaub ntawv xws li cov vuas ceramic. Lub tshuab hluav taws xob kiln yog qhov txuas ntxiv mus tua cov roj, uas siv cov hlau uas tig rov qab los ua tus cab kuj ntawm billet. Cov khoom lag luam ceramic tau tso rau ntawm ntau cov kab rov tav hluav taws-tiv thaiv nrog qhov ntom ntom, thiab qhov kev sib hloov ntawm cov yob tuaj yeem ua kom cov ceramic xa los ntawm lub taub hau kiln mus rau kiln tus Tsov tus tw. Yog li ntawd, cov menyuam lub qhov cub hu ua menyuam cov menyuam kiln, uas feem ntau muaj qhov ntu me me thiab qhov kub tsis sib xws hauv qhov cub, yog li nws tsim nyog rau kev tua hluav taws sai, tab sis cov khoom siv rau cov menyuam thiab kev teeb tsa kev tseev kom muaj. Nws yog tsuas yog siv rau kev tua hluav taws sai ntawm lub tsev cov khoom ntxuav tais diav.
Lub puab phab ntsa qauv ntawm cov menyuam lub plhaw plhaub yog tsim los ntawm cov txheej txheem ko taw pob zeb, ntau txheej txheej refractory cib, tiaj tus hlau thiab mullite cov menyuam lub pob zeb nrog cov menyuam ntxig rau. Vim tias mullite cov menyuam lub qhov taub cib ua rau lub siab ntawm qhov hnyav ntawm ntau txheej txheej refractory cib, koov ko taw pob zeb thiab koov cib, thiab lub qhov cub muaj qhov kub siab, nws yooj yim ua rau cov tiaj tiaj steel khoov, yog li qhov nyhav ntawm refractory cib saum toj no nws tau mloog zoo ntawm lub qhov av cib, feem ntau ua rau cov khoom tawg lossis cov khoom tawg hauv lub pob zeb, uas ua rau nws tsis yooj yim rau cov menyuam ua haujlwm khiav lag luam ib txwm.
Cov khoom yog cim los ntawm lub zog kub, lub zog thermal poob siab, siab kub nkag tsis kam, muaj zog oxidation tsis kam thiab zoo hnav tsis kam. Nws yog siv rau hauv cov menyuam ncu xws li niaj hnub ceramics, tu cev ceramics, lub tsev ceramics thiab cov ntaub ntawv sib nqus. Nws yog qhov zoo tshaj plaws kiln rau qhov kub kub hluav taws kub ua haujlwm.