Oct 07, 2024

High hnav-resistant thiab tshav kub-resistant siab alumina cib, uas suav nrog kev sib sau ua ke ntawm {} mm alum,} mm alum,}} ntu ntawm nplua Hmoov rau Alum, {9}}}}}} mud, {}}}}}}} cov dej. High hnav-resistant thiab tshav kub-resistant siab alumina muaj lub zog siab, hluav taws kub tiv taus, thiab cov kev coj ua kom tsis kam thiab thermal poob siab kuj. Haum rau kev ncig ua si lub txaj boiler cyclone separator ncaj, cyclone separator ncaj qha seem seem thiab cook, rov qab muaj cua sov, metallurgical muaj cua sov thiab lwm yam khoom siv thermal.
Cov yam ntxwv ntawm kev hnav siab hnav-resistant thiab tshav kub-resistant siab alumina cib
1. Hluav Taws Kub Tsis kam
High Alumina Crick cov khoom yog ntau yam ntawm alumina silicate regractory, thiab lawv cov ntsiab lus nce ntxiv nrog kev nce qis dua {2}} degree. Corundum cib nrog AL2O cov ntsiab lus ntau dua 95% tuaj yeem muaj kev ua kom tiav ntawm {{6} degree.
2. Thauj cov khoom so
Lub load softening kub ntawm high alumina cov khoom siv alumina siab zuj zus nrog cov ncauj lus loj thiab cov duab av alkali thiab ntau dua li 1420-1530 degree. AL2O3. Corundum cib nrog cov ntsiab lus ntau dua 95% muaj lub thauj khoom softening kub tshaj 1600 degree.
3. Slag Kuj
Vim yog cov ntsiab lus nruab nrab thiab cov ntsiab lus siab ntawm txhuas oxide nyob rau hauv high cov khoom siv high alumina, cov ntaub ntawv muaj peev xwm tiv thaiv cov yaig ntawm acidic thiab alkaline slag.
4. Thermal poob siab ruaj khov
Nyob rau hauv high alumina cib zaub siab, kev nyuaj siab concentration tshwm sim vim muaj kev nthuav dav thaum ntsuas kub ntawm refractory cib hloov. Yog li, lub thermal poob siab ntawm high alumina cov khoom siv cib siab yog qhov phem tshaj li cov dej txias feem ntau tsuas yog {3-5 lub sij hawm.
5. Reburning kab hloov
Yog hais tias lub cub hluav taws kub ntawm cov khoom loj uas muaj txiaj ntsig zoo thiab lub sijhawm hluav taws muaj zog thiab lub ntim ruaj khov yog qhov sib txawv thiab cov kab sib tua yuav me; Ntawm qhov tsis sib xws, seem ntawm shrinkage xws li ntawm av nplaum cib cov khoom yuav tshwm sim, uas tseem tshwm sim los ntawm recrystallization.

High hnav-resistant thiab tshav kub-resistant siab alumina cicks yog siv rau hauv cov tshuab hluav taws kub, hluav taws xob rauv taws, cov hluav taws xob hluav taws xob hluav taws xob, thiab cov hluav taws kub.
 

 

 

 

 

 

 