Graphite electrodes ua li cas

Sep 13, 2022

1.Processing daim ntawv ntawm graphite khoom

Muaj peb txoj hauv kev ua haujlwm tseem ceeb ntawm graphite electrode: txoj kev vibration siab, NC tsis siv neeg txoj kev tsim thiab cov txheej txheem ua tshuab.

(1) Pressurized vibration method: lub pressurized vibration method yuav tsum muaj ib lub tshuab tshwj xeeb, thiab cov duab ntawm electrode niam pwm yog opposite rau cov electrode. Cov ntaub ntawv graphite thiab cov cuab yeej tsim yuav tsum muab tso rau ib leeg thaum ua tiav, tawm hauv qhov sib txawv. Cov kua machining muaj li ntawm dej thiab abrasive yog txhaj rau hauv lub workpiece. Cov graphite thiab cov cuab yeej tsim yog ultrasonically vibrated thaum dhau los ntawm cov kua machining. Nyob rau hauv qhov kev txiav txim ntawm abrasive cuam tshuam quab yuam, graphite yog tev tawm me ntsis los tsim cov duab uas xav tau. Cov abrasive yog SiC, B4C lossis pob zeb diamond. Lub coarser lub abrasive, qhov ceev ntawm machining ceev. Thaum lub tshuab cuab yeej ua haujlwm, nws txais yuav hom kaw thiab cov ntaub thaiv dej rau kev ua haujlwm. Nws yog tsim rau EDM hauv kev tsim khoom loj.

(2) NC tsis siv neeg txoj kev tsim: NC tsis siv neeg txoj kev tsim yuav tsum tau tshwj xeeb graphite electrode txoj kev tshuab. Nws txais NC hom thiab muaj cov cuab yeej hloov pauv tsis siv neeg, uas tuaj yeem ua raws ntau yam cuab yeej. Txhawm rau txhim kho kev ua haujlwm ib puag ncig, graphite electrode yog ib puag ncig los ntawm cov ntaub thaiv dej kom tiv thaiv graphite plua plav tawm ntawm txhua qhov chaw. Tsis tas li ntawd, cov txheej txheem ntub dej tuaj yeem siv tau, thiab cov dej-soluble txiav cov kua tuaj yeem tiv thaiv cov cuab yeej los ntawm kev hnav thiab cov graphite plua plav ya. Lub tshuab cuab yeej muaj cov cuab yeej lim dej ua haujlwm siab, uas tuaj yeem cais cov kua txiav thiab graphite chips, thiab xyuas kom muaj kev ua haujlwm ntev. Nws yog cov cuab yeej tshwj xeeb zoo tshaj plaws rau kev ua cov graphite electrode, thiab tsim nyog rau kev ua cov electrode tuag. Txawm li cas los xij, nws tus nqi siab thiab nws daim ntawv thov hauv Suav teb tsis yog universal.

(3) Machining txoj kev: machining txoj kev yog lub ntsiab txoj kev saws los ntawm domestic general pwm manufacturers.

Graphite cov ntaub ntawv tuaj yeem ua tiav los ntawm kev tig, milling, drilling thiab sib tsoo. Tsis tas li ntawd, graphite cov ntaub ntawv yog nquag ya tshauv thaum lub sij hawm machining, uas muaj kev cuam tshuam tsis zoo rau cov khoom siv thiab cov neeg ua haujlwm.

2.Cov txheej txheem ntawm cov khoom siv graphite

(1) Graphite yog immersed hauv roj. Cov ntaub ntawv graphite yuav tsum tau muab tso rau hauv cov roj cav rau kaum teev ua ntej machining, kom cov roj tuaj yeem nkag mus rau hauv cov ntaub ntawv graphite, kom cov hmoov tshauv tsis ya thaum lub tshuab ua haujlwm thiab tau txais qhov chaw du.

(2) Xim kab. Tom qab qhov kev ntxhib los mos ntawm cov txheej txheej ntawm cov electrode, ib txheej nyias ntawm cov xim dawb yuav tsum tau muab txau rau ntawm qhov chaw kos npe, kom cov kab no meej thiab yooj yim rau kev ua haujlwm.

(3) Machining yog ua.