I. Ua rau kev tawg ntho ntawm castable refractory rau cement kiln
1 Vim muaj cov haujlwm ntau heev, feem ntau cov cement nroj tsuag yuav tsum siv sij hawm los ua txuj ua tus kho. Yuav kom qhib lub kiln ntau li sai tau, qhov kho thiab ci lub sij hawm ntawm cov castables yuav tsum tau compressed.
2 tam sim no, Tuam Tshoj tus cement kiln refractory castable khoom yog SiO2, Al2O3, thiab nws cov binder yog ceev ceev-hardening ntxov-zog MAAAC raws aluminate MAAs. Qhov no yuav tsum tau hais tias cov castables muaj sij hawm txaus curing thiab ib qho kev tsim nyog ci tom qab kev tsim kho, uas yuav siv sij hawm ntev.
3 Tuam Tshoj txoj kev txhim kho kev lag luam hauv kev lag luam yog tsim los ntawm lub chaw taws ua haujlwm rau lub tshuab ua kom sov, cov neeg ua haujlwm ntawm kev tsim kho, seb qhov kev tsim kho puas yog muaj kev cuam tshuam zoo dua rau kev tsim kho thiab siv cov khoom siv hluav taws xob.
4 Qee qhov tshwj xeeb ntawm cov cement kiln, xws li lub hauv ntej qhov ncauj qhov ntswg, lub hau npog lub taub hau, sab saum toj ntawm lub txaj txias thiab sab phab ntsa, thiab lwm yam, muaj qhov teeb meem ntawm kev nyuaj rau hauv ci. Rau cov khoom no, qee cov chaw lag luam luam tsis tau ntoo ci txhua qhov, thiab qee lub tuam txhab tsuas ua ci rau ib lub sijhawm luv luv. Nyob hauv qhov kub hnyiab kiln theem, vim kev tswj ntawm cov cement kiln tsis yog, cov roj kub ntws propagates thiab radiates rau lub kaw lus kiln ntawm ib yam ceev, thaum lub taub hau lub taub hau thiab qhov txias txias tsuas muaj ib feem ntawm cov hluav taws xob hluav taws xob lub zog, uas yog tsis txaus rau hauv tshav kub. Yuav kom tag nrho tso dej dawb hauv lub castable. Thaum pib ntawm cov khoom, cua kub hauv lub cev rov mus rau lub taub hau kiln hauv ib lub sijhawm luv; nyob rau tib lub sij hawm, lub siab kub clinker (saum toj siab 1300 ° C) pib pib nyob rau hauv qab ntawm lub cover kiln, ua rau kub ntawm lub taub hau lub taub hau thiab lub grate txias kom nce sharply. Nyob rau lub sij hawm no, qhov tshwm sim uas cov ntaub ntawv castable thiab ntog tawm yog feem ntau yuav tshwm sim.
2. Mechanism tsom xam ntawm kev tawg ntawm cov pob zeb tawg ua rau cement kiln
Tam sim no, lub npog lub taub hau ntawm Cement ntau lawm kab hauv Suav teb, qhov kub kub ntawm lub taub txias txias thiab cov khoom castable ntawm lub qhov ncauj hauv qhov ncauj yog nquag tawg. Yog vim li cas qhov kev soj ntsuam, feem ntau yog nyob rau hauv lub kwj phaus, vim tias qhov kub hlob tuaj sai heev, qhov kub nyob hauv lub kiln tsuj sai, cov dej dawb hauv cov khoom siv hluav taws xob hloov ntawm kua mus rau lub sijhawm luv, lining kub nce. Vapor siab, thaum cov pa dej hauv sab hauv lub qhov quav tsis muaj zog nyob rau lub sijhawm, lub siab yuav nce. Thaum cov dej tsis muaj zog hauv sab hauv lub qhov quav yog tawm ntawm qhov sib npaug, qhov tshwm sim ntawm kev sib tawb, kab xev thiab xuas nrig ntawm lub castable yuav tshwm sim.
Rau qhov teeb meem ntawm tawg ntawm castables, refractory manufacturers ntawm xis mas kiln feem ntau siv 0.1% rau 0.3% ntawm cov organic fibers nyob rau hauv lub lag luam kev lag luam los tiv thaiv qhov tshwm sim ntawm tawg. Cov kua roj organic yog yaj lossis hlawv thaum txog 160 ° C los ua ib qho zoo thiab nqaim pore uas cuam tshuam thiab sib npaug sib npaug. Tus tsim ntawm cov organic fiber ntau dua cov roj permeability ntawm cov khoom siv hauv tsev, accelerates lub kua thiab buffers tus dej vapor siab, thiab tiv thaiv ci thiab qhib. Qhov kev hloov ntawm nws lub cev hloov ntawm qhov kev tuag yog qhov ua rau lub hauv siab tawg. Txawm li cas los, kev siv cov organic fibers muaj teeb meem nyob rau hauv qhov castable yog tsis yooj yim dispersed, tus nqi ntawm ntxiv yog loj, thiab lub zog yog cuam tshuam.
3. Ntsuas los daws qhov teeb meem ntawm kev tawg ntawm cov pob zeb tawg ua rau cement kiln
1Tau vim txhua lub tuam txhab muaj cement cog qoob loo muaj kev sib txuas ntawm cov khoom siv, kev siv cov khoom siv thiab lwm cov khoom thaum lub sijhawm kho, txhua lub tuam tsev yuav tsum sib koom tes thiab ua cov txheej txheem tsim ntawm cov khoom ntim rau hauv txhua feem ntawm cov cement kiln. Rau qee cov ntaub ntawv pov thawj uas tsis yooj yim rau chiv (txias txias, lub khob ntawm lub qhov khaus thiab lub qhov ncauj), qhov muaj feem thib yuav tsum tau muab rau cov dej ntws siv, thiab yuav tsum tau cure sij hawm txaus; tib lub sijhawm, kev saib xyuas ntawm kev tsim kho lub tsev yuav tsum ua kom zoo, thiab sib xyaw cov castables yuav tsum tau ua. Qhov dej ntxiv ntxiv, daim formwork, thiab kev txij nkawm yuav tsum ncaj qha raws li cov lus qhia kev tsim kho.
2 Thaum lub hau khwb taub hau ua lub tsev, nws yog qhov zoo tshaj kom tawm hauv lub qhov quav. Qhov kev yuam kev yuav tsum yog: 300 hli × 300 hli, thiab kos nrog φ5mm ntoo sawb, qhov tob yog ib nrab ntawm cov castable.
3 Tom qab lub qhov kaw qhov thaiv qhov kaw lawm, cia 8 lub qhov thiab qhov tsis muaj dej tsis huv. Nyob rau tib lub sij hawm, yuav kom ntseeg tau hais tias lub plhaub av nplaum nyob hauv lub qhov ncauj ua ntej lub qhov ncauj tsis ntog thaum ci, nws yog qhov zoo uas siv cov ≈3 hli xyaw lo rau lub qhov tso rau hauv qhov kev tsim kho. Qhov chaw dim pa yog nyob ntawm 100 square metres ib square meter.
4 Kev kho thiab kho dua ntawm cov pob zeb cement, ua ntej siv cov roj hlawv roj av, qee qhov tshwj xeeb (lub hau npog lub taub hau, lub qhov cub txias kom txias, lub qhov ncauj rau qhov ntswg) zoo tshaj plaws ci nrog ntoo, thiab lub sij hawm ci tsis pub tsawg tshaj 12 . Nyob rau tib lub sij hawm, nyob rau hauv tus txheej txheem ntawm ziab lub kiln, lub cua sov tus nqi yuav tsum tsis txhob yuav sai heev. Rau cov low-cement series refractory castables, thaum lub thickness ntawm meem yog nyob rau hauv 200-400mm, qhov zoo tshaj yog cua sov tus nqi tsis ntau tshaj 15 ° C ib teev twg. xav tau.
5 Thaum kho qhov xwm txheej ceev, kev raug mob nkawm tsis muaj lub sijhawm ci ntsa iab, phosphate-bonded refractory castables, xws li PA-852 phosphate castables, yuav siv tau. Cov khoom no muaj qhov kom zoo dua uas tsis pub ci, thiab lub zog nce ntxiv tuaj raws li qhov ntsuas kub nce. Txawm li cas los xij, nws yuav tsum tau taw qhia tias hom khoom ntawm no kuj muaj nws tus kheej qaug zog, xws li kev txom nyem hnyav thiab kev pab cuam luv luv lub neej.
Hauv ntej, qhov teebmeem ntawm qhov teeb meem tawg ua rau cement kiln yog ib qho nyuaj, uas yog muaj feem xyuam nrog ntau yam, tshwj xeeb tshaj yog nyob rau lub caij ntuj no. Ntxiv 0.1% mus rau 0.3% ntawm cov fwj siv tawg-tawg mus rau castable tuaj yeem txhim kho kev tawg ntawm qhov khoom. Rau qhov hauv ntej lub qhov ncauj, lub taub txias, lub hau khi, thiab lwm yam khoom, qhov chaw uas cov khoom ntim yuav tawg ntho, tsuav yog kev tsim kho, qhov zoo ntawm txoj kev tsim kho, qhov cua, qhov ci, lub qhov tho qhov laj kab tawg yog qhov tshwm sim Qhov tshwm sim tsis zoo tag nrho.