Dec 28, 2023

Ib, Ntawm qhov chaw cia khoom thiab npaj cov cuab yeej

1. Cov khoom sib xyaw qhuav qhuav thiab ntim khoom yuav tsum raug thauj mus rau qhov chaw tsim kho. Nws yog nruj me ntsis txwv tsis pub muab lawv tso rau hauv qhov qhib cua. Kev ntsuas dej los nag thiab dej noo yuav tsum tau ua, thiab cov ntaub ntawv uas tsis tau ntim yuav tsum tau siv sai li sai tau. Nws tsis pub tshaj 6 teev nyob rau lub caij ntuj no thiab 4 teev nyob rau lub caij ntuj sov. Yas uas raug los nag lossis dej noo yog txwv tsis pub siv.

High aluminium, high-strength, hnav-resistant yas yuav tsum tau rammed nrog ib tug roj hmab rauj, thiab kev tsim kho machinery yuav tsum muaj ib tug quab yuam rau kev sib tov, xws li ntsuas cov thoob, nplais, trimming riam, hlau txhuam, thiab lwm yam.

2, Plastic mix ratio

100kg ntawm yas, 7-8kg kua txhuas dihydrogen phosphate binder, thiab cais ntim ntawm coagulants yuav siv tau. Thaum qhov kub siab tshaj 30 degrees Celsius, nws tuaj yeem txo qis raws li qhov tsim nyog. Raws li qhov loj ntawm lub tov khoom, qhov sib tov yog hloov proportionally thiab txiav txim siab ntawm qhov chaw. Tus neeg mob siab rau yog lub luag haujlwm saib xyuas cov khoom sib piv, ntsuas, thiab kev sib xyaw, thiab khaws cov ntaub ntawv ntawm txhua qhov sib tov.

3, Yas sib tov

1. Ua ntej sib tov, ntxuav lub tov khoom thiab ua kom cov khoom huv si.

2. Ua ntej, ntxiv granular qhuav yas thiab do li 2 feeb. Do cov agglomerated loj hais sib nrug, thiab ces maj mam thiab sib npaug ntxiv cov binder ib zaug. Lub sijhawm stirring yuav tsum tsis pub tsawg tshaj 5 feeb. Tom qab ntawd, sib npaug ntxiv cov coagulant thiab do rau 1-2 feeb kom dhau los ua cov khoom siv yas uas yooj yim rau cov duab, thiab tom qab ntawd txuas nrog kev tsim kho.

Tom qab sib tov, cov ntaub ntawv yuav tsum tau ntim thiab thauj mus rau hauv lub hnab woven. Thaum qhov chaw ua haujlwm kub siab tshaj 25 degree, cov yas sib xyaw yuav tsum siv li ntawm 40 feeb. Nws tuaj yeem siv tau li ntawm 60 feeb thaum nws qis dua 25 degree

4, Kev xav tau rau kev tsim kho yas

1. txhuam asphalt pleev xim rau ntawm qhov chaw tsim kho, nrog cov yeeb yaj kiab tuab tsis pub tsawg dua 0.5mm (los yog raws li kev tsim qauv); Qhov saum npoo ntawm qhov chaw tsim kho yuav tsum tsis muaj av, plua plav, thiab lwm yam khib nyiab. Cov yas tuaj yeem siv tau tsuas yog tom qab cov xim asphalt qhuav tag, thiab dej yog nruj me ntsis txwv tsis pub cov yas tom qab kev tsim kho.

2. Nws yuav tsum tau ua kom compact thiab theem ntawm qhov chaw. Yog hais tias muaj ib tug tsa ceg, nws yuav tsum tau leveled nrog ib tug trimming riam thiab xyuas rau flatness nrog ib tug pas ntsuas. Yog tias pom tias qhov tuab tsis txaus, nws yog ib qho tsim nyog yuav tsum tshem tawm li ib feem peb ntawm cov tuab, rov ua dua, thiab sib cog lus kom tiv thaiv cov khoom los ntawm kev poob hauv txheej thaum lub sijhawm ua haujlwm boiler.

3. Yas expansion pob qij txha yuav tsum tau preset raws li kev cai tsim.

4. Qhov siab tshaj plaws kev tsim kho thickness ntawm yas yuav tsum tsis pub tshaj 150mm.

5. Tom qab kev tsim kho, cov yas tuaj yeem siv los khi cov dej ntub dej nrog cov xaim hlau, nrog rau qhov sib nrug ntawm 200 × 200mm thiab ci.

Cov thauj tog rau nkoj hauv cov yas yuav tsum tau ua los ntawm cov hlau tsis muaj cua sov, thiab cov khoom siv rau qhov kub thiab txias hauv 900 degrees yuav tsum tsis txhob qis dua 1Cr18Ni9Ti.

5, Yas curing

Thaum lub sijhawm tsim kho, kev co ntawm lub cev uas twb tau tsim lawm yuav tsum zam kom ntau li ntau tau. Tom qab kho qhov chaw ua haujlwm ntawm lub hauv ob sab phlu, kev kho ntuj yuav tsum tau nqa tawm ntawm qhov kub ntawm 15-35 degree . Hauv qhov chaw qhuav (nrog cov av noo tsis tshaj 70%), lub sijhawm kho ntuj yog 5-7 hnub. Tom qab ntawd, lub qhov cub tuaj yeem qhuav raws li qhov cub nkhaus.

6, Kho cov kab nrib pleb nyob rau hauv pem hauv ntej ntawm lub qhov cub yas

Thaum cov kab nrib pleb dav ntawm cov yas hauv ob sab phlu tsis nthuav dav yog ntau dua 1 hli ua ntej ziab, nws yuav tsum tau kho; Thaum qhov dav ntawm qhov tawg yog 1-3 hli, txoj kev sau cov kab nrib pleb tuaj yeem siv tau, uas yog tshuaj tsuag kua nplaum ntawm qhov tawg kom mos thiab maj mam kais nrog roj hmab rauj kaw qhov tawg lossis ncaj qha sau. nws nrog softer yas; Thaum cov kab nrib pleb loj dua 3 hli, cov yas tawg yuav tsum tau khawb rau hauv ib lub qhov ncauj zoo li lub qhov ncauj nrog ib txoj kab uas loj sab hauv thiab sab nraud me me, txau nrog cov kua nplaum kom mos thiab moisten, thiab ua tib zoo ntim cov yas.

 

 

 

 

 

 

 