Magnesium carbon cib yog tsim los ntawm high melting point alkaline oxide magnesium oxide (melting point 2800 degree) thiab siab melting point carbon cov khoom uas nyuaj rau infiltrated los ntawm slag, nrog rau ntau yam uas tsis yog oxide additives ntxiv. Cov khoom siv hluav taws xob tsis kub hnyiab tau ua los ntawm kev sib xyaw carbonaceous binders. Magnesia carbon bricks yog siv rau hauv ob sab phlu converters, AC arc rauv, DC arc rauv, slag kab hauv steel ladles, thiab lwm yam.
Magnesia carbon cib, raws li cov khoom sib xyaw refractory, zoo siv lub zog slag yaig tsis kam ntawm magnesia xuab zeb thiab thermal conductivity thiab tsis tshua muaj expansion ntawm carbon, compensating rau qhov loj tshaj qhov tsis zoo ntawm cov tsis zoo spalling tsis kam ntawm magnesia xuab zeb.
Nws cov yam ntxwv tseem ceeb muaj xws li: qhov kub thiab txias tsis kam, muaj zog slag tsis kam, zoo thermal poob siab tsis kam, thiab qis siab - kub nkag.
Cov txheej txheem ntau lawm
Cov khoom nyoos
Cov ntaub ntawv tseem ceeb rau MgO-C cib suav nrog fused lossis sintered magnesia, flake graphite, organic binders, thiab antioxidants.
Magnesia xuab zeb
Magnesia xuab zeb yog cov khoom siv tseem ceeb rau kev tsim MgO-C cib, uas tuaj yeem muab faib ua fused magnesia thiab sintered magnesia. Piv nrog rau sintered magnesia, fused magnesia muaj qhov zoo ntawm coarse spinel nplej thiab siab particle ntim ntom ntom, thiab yog cov khoom siv tseem ceeb siv hauv kev tsim cov magnesia carbon cib. Txhawm rau tsim cov ntaub ntawv zoo tib yam magnesia refractory, cov ntsiab lus tseem ceeb rau cov khoom siv magnesia yog qhov kub thiab txias thiab corrosion kuj. Yog li ntawd, kev saib xyuas yog them rau purity ntawm magnesia thiab C / S piv thiab B2O3 cov ntsiab lus nyob rau hauv nws cov tshuaj muaj pes tsawg leeg. Nrog rau txoj kev loj hlob ntawm metallurgical kev lag luam, smelting tej yam kev mob yog nce stringent. The magnesia used in MgO-C bricks applied in metallurgical equipment (converters, electric furnaces, ladles, etc.) not only requires high density and large crystallinity in terms of chemical composition, but also in terms of organizational structure.
Carbon qhov chaw
Txawm nyob rau hauv ib txwm MgO-C cib los yog dav siv tsawg-carbon MgO-C cib, flake graphite feem ntau yog siv los ua nws cov pa roj carbon. Graphite, raws li cov khoom siv tseem ceeb rau kev tsim MgO-C cib, feem ntau tau txais txiaj ntsig los ntawm nws lub cev zoo heev: ① tsis ntub dej rau slag. ② High thermal conductivity. ③ Tsawg thermal expansion. Tsis tas li ntawd, graphite thiab cov khoom siv refractory tsis dhau eutectic ntawm qhov kub thiab txias, ua rau muaj kev kub ntxhov siab. Lub purity ntawm graphite muaj qhov cuam tshuam loj rau kev ua haujlwm ntawm MgO-C bricks. Feem ntau, graphite nrog cov ntsiab lus carbon ntau dua 95%, nyiam dua ntau dua 98%, yuav tsum tau siv.
Ntxiv nrog rau graphite, cov pa roj carbon dub kuj yog siv los tsim cov magnesia carbon cib. Cov pa roj carbon dub yog cov khoom tawg yooj yim heev ntawm cov hmoov carbonaceous uas ua los ntawm thermal decomposition lossis tsis tiav combustion ntawm hydrocarbons. Cov pa roj carbon dub yog me me (tsawg dua 1 μ m), nrog rau thaj tsam loj, cov pa roj carbon ntau ntawm 90-99%, siab purity, siab hmoov resistivity, siab thermal stability, thiab thermal conductivity tsawg, ua rau nws nyuaj rau graphitize carbon. Qhov sib ntxiv ntawm cov pa roj carbon dub tuaj yeem txhim kho cov khoom tiv thaiv kev tshem tawm ntawm MgO-C cib, ua kom cov pa roj carbon ntau ntxiv, thiab ua kom cov cib kom ceev.
Binder
Cov binders uas nquag siv los ua MgO-C cib muaj xws li coal tar, thee tar pitch, petroleum asphalt, asphalt tshwj xeeb carbonaceous resins, polyols, asphalt modified phenolic resins, synthetic resins, thiab lwm yam. Muaj ntau ntau hom binders siv:
1) Cov khoom siv asphalt. Tar asphalt yog cov khoom siv thermoplastic uas muaj kev sib raug zoo rau graphite thiab magnesium oxide, cov pa roj carbon ntau seem tom qab carbonization, thiab tus nqi qis. Nws tau siv dav hauv yav dhau los; Txawm li cas los xij, tar pitch muaj carcinogenic aromatic hydrocarbons, tshwj xeeb tshaj yog qib siab ntawm benzo [b] pyrene; Vim muaj kev txhawb zog ntawm ib puag ncig kev paub, kev siv tar pitch yog txo tam sim no.
2) Resin raws li cov khoom. Synthetic resin yog tsim los ntawm cov tshuaj tiv thaiv ntawm phenol thiab formaldehyde, thiab tuaj yeem sib xyaw zoo nrog cov khoom refractory ntawm chav tsev kub. Tom qab carbonization, cov seem ntawm cov pa roj carbon ntau yog siab, thiab tam sim no nws yog lub ntsiab binder siv nyob rau hauv zus tau tej cov MgO-C bricks; Tab sis cov txheej txheem iav iav tsim tom qab carbonization tsis zoo rau cov thermal shock thiab oxidation tsis kam ntawm cov ntaub ntawv refractory.
3) Ib yam khoom tau los ntawm kev hloov kho asphalt thiab resin. Yog tias lub binder tuaj yeem tsim cov qauv embedded thiab hauv -situ carbon fiber cov ntaub ntawv tom qab carbonization, ces tus binder no yuav txhim kho qhov siab -kub kev ua tau zoo ntawm cov ntaub ntawv refractory.
Antioxidant
Txhawm rau txhim kho oxidation tsis kam ntawm MgO-C cib, cov khoom siv me me feem ntau tau ntxiv. Cov tshuaj ntxiv muaj xws li Si, Al, Mg, Al Si, Al Mg, Al Mg Ca, Si Mg Ca, SiC, B4C, BN, thiab tsis ntev los no tau tshaj tawm Al-B-C thiab Al-SiC-C systems. Lub hauv paus ntsiab lus ntawm kev ua ntawm additives tuaj yeem muab faib ua ob yam: ntawm ib sab, los ntawm qhov kev xav ntawm qhov ntsuas kub, uas yog, ntawm qhov ua haujlwm kub, cov khoom siv ntxiv lossis cov khoom ntxiv tuaj yeem ua rau cov pa roj carbon monoxide los ua lwm yam, uas muaj kev sib raug zoo rau cov pa ntau dua li cov pa roj carbon monoxide thiab cov pa roj carbon monoxide, thiab ua ntej tshaj carbon oxidation los tiv thaiv carbon; Ntawm qhov tod tes, los ntawm qhov kev xav kinetic, cov khoom ntxiv tuaj yeem ua rau O2, CO, lossis carbon los tsim cov tebchaw uas hloov cov microstructure ntawm cov khoom siv refractory, xws li nce ntom, thaiv qhov hws, thiab cuam tshuam cov diffusion ntawm oxygen thiab cov khoom siv tshuaj tiv thaiv.