Environmentally production magnesia alumina carbon brick is a refractory brick developed and produced to improve the user's oven drying environment and use environment. Based on the production process of magnesia alumina carbon brick, two improvements have been made. First, the binder has been changed to environmentally friendly resin, which is free of phenol and formaldehyde. There is no harmful gas during oven drying and use, which is not harmful to people and the environment. Second, the baking temperature is increased and a small amount of odor is discharged. After testing and user application, the environmental protection magnesium chromium brick has no harmful smell and improves the environment. At the same time, the environmental protection magnesium aluminum carbon brick has lower porosity, higher compressive strength, stronger slag erosion resistance and better use effect than the original product.