Cov Txheej Txheem Ntau Lawm thiab Daim Ntawv Thov Ntawm Polycrystalline Mullite Refractory Fibers

Dec 03, 2024

Polycrystalline fiber ntau tam sim no cov hom ultra tshiab kub siab-kub refractory khoom hauv Suav teb. Nws muaj cov yam ntxwv ntawm lub teeb ntom ntom, siab thermal kuj, thermal sib txawv, qis kev khiav hauj lwm kub, thiab zoo zog-txuag nyhuv.

Cov txheej txheem ntau lawm ntawm polycrystalline mullite fiber ntau

Polycrystalline Mullite Fibers yog tsim los ntawm cov qauv tshuaj colloid. Kev tsim khoom lag luam yog los ua soluble aluminium thiab silicon ntsev rau hauv kev daws colloidal nrog qee yam viscosity. Cov kev daws teeb meem colloidal yog spun mus rau hauv fiber ntau embryos los ntawm centrifugal spinning txoj kev, thiab tom qab ntawd hloov mus ua kev kho cua sov li-kub.

Cov khoom siv refractory siv los tsim lub zog hluav taws xob yog ib qho tseem ceeb rau kev siv hluav taws xob ua haujlwm thiab kev pabcuam lub neej ntawm cov kiln. Tam sim no, feem ntau cov kev muaj kub-kub-kub muaj zog hauv Suav teb siv refractory cib cas refractory cas, ramming cov ntaub ntawv, thiab lwm yam ntaub ntawv los tsim cov cua sov lub cev. Txawm li cas los xij, muaj kev tsis zoo xws li luv pab lub neej, kev siv hluav taws xob tsis zoo, kev siv hluav taws xob siab, thiab hnyav hnyav. Yog li no, kev siv refractory fibers raws li txoj kev rauv rauv yog ib qho kev rov ua dua tshiab mullite fibers yog cov khoom siv hluav taws xob zoo tshaj plaws rau cov khoom siv hluav taws xob rau hauv cov khoom siv hluav taws xob.

The application of polycrystalline mullite fibers can be achieved through several methods such as pasting, masonry, splicing, hanging, and tiling. Firstly, sib txawv kev pab txoj kev pab yuav tsum tau txais raws li cov xwm txheej tshwj xeeb ntawm lub KILN. Siv polycrystalline mullite cov paj rwb rew los tsim sib txawv cov lus ntawm cov khoom lag luam: relt, cib, raj, khoom, thiab lwm yam, thiab lwm yam

 

 

 

 

 

 