Muaj ntau yam ntxwv ntawm Cov Khoom Siv Castable High-strength, Koj Paub Txog Ib Tug Neeg

Jan 21, 2019

Yuav kom txhim khu lub zog ntawm castable thiab txhim kho kev lag luam ntawm txhuas-silicon castable, cov nram qab no cov kev ntsuas raug coj (ntawm no xa mus rau cov cement raws li castables):

(1) Matrix muaj pes tsawg leeg. Matrix muaj pes tsawg leeg muaj kev txuam tseem ceeb ntawm kev siv kub, kev kho siab kub thiab khoom sintering ntawm castable. Lub matrix yuav tsum ua raws li bauxite clinker nrog tsawg K2O thiab Na2O cov ntsiab lus, tswj cov nyiaj ntawm cov maas ntxiv, optimize cov khoom xyaw, thiab ua tus duab ntawm castable kwv yees rau cov tshuaj muaj pes tsawg leeg ntawm mullite (A3S2). Ntawd yog, cov ntsiab lus ntawm Al2O3 thiab SiO2 nyob rau hauv daim phiaj siv khoom yog kho kom tsim ib micro-expansion ntawm mullite ntawm qhov kub ntawm enthalpy kom zoo thermal poob siab thiab lub zog high-kub.

(2) Tus neeg saib xyuas kev ruaj ntseg. Ntshiab calcium aluminate cement yog siv los ua cov pob. Nws qhov tseem ceeb yog Cao · Al2O3 (calcium aluminate decomposition temperature yog 1600 ° C, qhov kev ua si yog siab heev, qhov kev sib tw ceev yog qhov qub, qhov ceev ceev yog ceev, lub zog thaum ntxov, siab zog nce tsis pom tseeb; • 2Al2O3 (calcium aluminate, decomposition temperature 1762) ° C) Cov dej thiab qhov ceev tau qeeb qeeb, lub zog thaum ntxov yog tsawg, thiab lub zog qeeb yog 髙. Los ntawm cov dej hla thiab qhov sib xyaw ntawm cov cement, cov aggregate thiab hmoov yog cemented ua ke, thiab tus nqi ntxiv yog tsawg dua 5%.

(3) Ntxiv ib qho tsim nyog ntawm hmoov zoo. Qhov sib ntxiv ntawm cov micropowder tuaj yeem ua rau cov voj voos sib txuas hauv nruab nrab, txhim kho sab hauv, thiab tsim cov agglomeration thiab densification kom nws ntom; tib lub sij hawm, nws tuaj yeem ua kom zoo dua qub thiab txo cov dej siv ntau dua. Nyob rau ntawm 110 ° C, 24 h nws ntxiv cov nyiaj ntau tshaj 8%, lub plhaub zais tau ntxiv, qhov tawg yog ntau tshaj, 4% 5% yog tsim nyog, lub zog ntawm cov khoom sib txawv ntawm cov kab micronized.

(4) Dispersing tus neeg sawv cev. Ntxiv cov nqi ntawm cov dej dispersant (dej txo tus neeg sawv cev tuaj yeem txhim kho cov dispersions zoo hmoov hmoov hauv castable, nce qhov kev ncua deb ntawm cov khoom, txo cov gravitation thiab txhuam, ntxiv kom fluidity ntawm castable, thiab cov dej dawb surrounded los ntawm cov particle Cov tshuaj pob txha los ua kom siv tau cov kua dej uas tsim tau thiab ua kom cov dej haus tsis tau siv Yog cov tshuaj sodium tripolyphosphate yog siv los ua tus dispersant, tus nqi ntxiv tsis txaus yog 0.05% mus 0.5%.

(5) Ntxiv ib tus neeg sawv cev. Cov khoom ntawm kyanite reacts nrog (Al2O3) nyob rau hauv cov hmoov kom tsim hom mullite (3Al2O3 • 2SiO2) los tsim volumetric micro-expansion kom offset lub shrinkage ntawm cov khoom kom zoo dua thermal poob hauj lwm. 3Al2O3 • 2SiO2 tuaj yeem tsim cov khoom tov nrog Fe203 thiab TiO2 rau hauv daim duab, uas tuaj yeem txo qhov nyiaj ntawm cov kub hauv siab kom nws qhov kev kub siab. Tus nqi ntxiv yuav tsum tsawg dua 10%.

(6) Kub nce qib. Corundum muaj cov yam ntxwv ntawm high melting point, ruaj khov thiab khoom kub zoo. Nws zoo dua yog siv tsawg dua 15% ntawm cov hmoov tsis tshua tshaj 0.088 hli.

(7) Siv dej haus. Tom qab castable qhuav lawm, cov khoom siv zog ntawm cov khoom no yog muab faib rau cov dej ntxiv rau kev tsim, thiab cov dej ntxiv yog 5%.