Lub ntsiab yam tseem ceeb cuam tshuam rau tus nqi creep ntawm Refractory cib nyob rau hauv kub kub ua hauj lwm ib puag ncig

Mar 11, 2026

Lub ntsiab yam tseem ceeb cuam tshuam rau tus nqi nkag ntawm refractory bricks nyob rau hauv kub kub ua hauj lwm ib puag ncig

Lub creep ntawm refractory cib yog qhov ua haujlwm ntawm qhov kub thiab txias, kev ntxhov siab, lub sijhawm, thiab cov khoom siv. Qhov siab dua qhov kub ntawm cov cib refractory tau muab tso rau, qhov ntau dua qhov kev ntxhov siab lawv tuaj yeem tiv taus, thiab lub sijhawm ntev dua, qhov nkag siab ntau dua.

Thaum refractory bricks yog tag nrho cov muaju, creep yog tsuas yog tswj los ntawm vacancy diffusion, dislocation txav, grain ciam ciam, thiab lub xeev bonding ntawm nplej, ntxiv rau yuav cuam tshuam los ntawm lub zog ntawm cov muaju muaj feem xyuam rau crystal elasticity. Cov khoom siv lead ua tsawg dua, cov ciam teb tsawg dua, thiab muaj zog sib cuam tshuam ntawm cov nplej, qhov tsis tshua muaj qhov hnyav yuav tshwm sim.
Thaum refractory bricks muaj iav theem Tshwj xeeb tshaj yog thaum lub iav theem yog ib ntus, cov creep ntawm refractory bricks yog tswj los ntawm iav theem. Lub iav ntau theem muaj thiab qhov qis dua qhov viscosity, qhov dej khov ntau tuaj yeem tshwm sim hauv cov cib refractory nyob rau hauv qis kev ntxhov siab, ua rau muaj kev nkag siab ntau dua ntawm qhov kub thiab txias. Thaum cov cib refractory muaj cov impurities uas yuav ua rau cov kua theem ntawm qhov kub thiab txias, ntau cov kua theem impurities raug tsim, xws li creep ntawm av nplaum cib, uas yog loj heev. Qhov nrawm dua qhov viscosity txo nrog qhov kub thiab txias, qhov creep hnyav dua.

Pores los yog kab nrib pleb ntawm cov ciam teb nyob rau hauv refractory cib tuaj yeem ua rau plam ntawm cov ciam teb. Tsis tas li ntawd, nyob rau hauv qhov kub thiab txias, cov kua theem hauv refractory cib tuaj yeem nkag mus rau hauv lub qhov hws hauv tib theem, tshwj xeeb tshaj yog rau hauv nruab nrab thiab me pores hauv qab 25 μ m. Yog li ntawd, lub hav zoov ntawm pores kuj cuam tshuam rau nkag los ntawm kev tsiv teb tsaws ntawm cov theem hloov pauv. Yog li, qhov pores ntawm refractory cib muaj qhov cuam tshuam loj rau kev nkag. Ua kom cov porosity ntawm refractory cib tuaj yeem ua rau lawv cov creep npaum li cas.