Aug 25, 2025

Alumina Sib Tsoo Pobyog spherical sib tsoo nruab nrab ua los ntawm cov ntaub ntawv raw xws li bauxite, cov hmoov alumina hmoov, thiab siab} kub pemin alumina hmoov. Nws yog feem ntau yog siv rau cov khoom crushing thiab ua hauv kev lag luam xws li metallurgy, sib tsoo, ua kom qhuav, thiab siab} kub recination. Raws li cov alumina cov ntsiab lus, nws tau muab faib ua nruab nrab cov khoom nruab nrab (60% {15%), ntawm cov 92 ceramics tau siv dav siv vim lawv qhov kev ua tau zoo. Aluminium oxide sib tsoo cov khoom muaj hnav-resistant thiab corrosion-resistant cov khoom, haum rau kev lag luam xws li cov khoom siv hluav taws xob thiab cov khoom siv hluav taws xob; Zosconia sib tsoo cov pob tau npaj los ntawm cov qauv nag los daus, nrog qhov tsis txaus ntseeg ntawm 6.1g / cm / cm thiab lub har thiab sib npaug ntawm 90, haum rau kev ua hmoov zoo.

 

Thaum lub sijhawm cov txheej txheem ntau lawm, iSostatic nias thiab tsawg {{{- kub ceev yog txo los ntawm kev ntxiv sintering kev pab cuam xws li y- psz. Nrog rau kev txo ntawm cov pob zeb zeb pob zeb, qhov kev thov txhua xyoo tau mus txog 50000 tons, uas ua lub luag haujlwm tseem ceeb hauv kev txhim kho kev sib tsoo ua kom zoo thiab cov khoom siv purity. NANO Alumina Sib tsoo Pob Txoj Haujlwm tau ua tiav txhua xyoo ntau lawm nplai ntawm 20000 tons. Cov khoom hloov kho cov khoom ntawm zirconia sib tsoo pob, silicon nitride sib tsoo nruab nrab, tau siv dav hauv kev sib tsoo hlau, uas tuaj yeem txo cov zog siv hluav taws xob los ntawm 40%

 

Alumina Sib Tsoo Pobyog ib hom tseem ceeb ntawm kev ua lag luam engamic thiab zwm rau siab - Tech cov khoom. Vim nws lub hardness haum, kev coj tawm hws, cov khoom siv ntawm cov hlau nplaum, thiab cov khoom siv hluav taws xob, cov khoom siv hluav taws xob, cov ntaub ntawv hluav taws xob, cov ntaub ntawv hluav taws xob, cov ntaub ntawv hluav taws xob, cov khoom siv hluav taws xob, cov xim hlau nplaum, thiab xim pleev xim rau. Lawv yog qhov siab-} zoo sib tsoo nruab nrab. Hauv kev lag luam architions ceramics, kev hnav muaj txiaj ntsig ntawm alumina cov pob ceramic muaj siab tshaj qhov ntawm ntuj flint thiab pebbles. Nrog rau kev txo qis ntawm high- zoo ntuj cov khoom siv thiab cov hnav zoo ntawm cov khoom nruab desamic, alumina cov khoom pob yuav nce ntxiv los ntawm cov ceramic manufacturers. Raws li cov ntsiab lus alumina sib txawv, lawv tuaj yeem muab faib ua nruab nrab cov pob alumina, nruab nrab cov pob loj alumina, thiab cov pob loj alumina. Feem ntau, peb cais cov nrog 60% cov ntsiab lus alumina alumina -80% cov ntsiab lus nruab nrab cov lus, thiab cov muaj ntau tshaj li 90% cov ntsiab lus alumina raws li cov pob alumina siab.

 

Alumina Sib Tsoo Pobyog muab faib ua ntej rau hauv 90 porcelain, 92 plooj (veneers), 95 plooj (veneers). Vim nws tus nqi tsim khoom heev, 99 plooj (99 porcelion) [1]
Nruab nrab cov khoom thiab nruab nrab cov pob zeb qub tau lees txais los ntawm feem ntau cov ceramic factories vim lawv tus nqi qis, tsuas yog siv rau kev sib tsoo cov kab ceramic cerams. High alumina pob yog dav siv nyob rau hauv lub precision thiab sib sib zog nqus, loj me me, mob siab heev, corrosion tsis kam, thiab tsis muaj kuab paug. Ntawm lawv, cov pob loj alumina nrog cov ntsiab lus ntawm 92 yog feem ntau siv.
 

 