Jun 16, 2026

Corundumyog cov ntxhia oxide tsuas yog tsim los ntawm alumina (Al2O3), nrog cov xim xws li tsis muaj xim lossis grey, daj grey, xiav, thiab lwm yam. Nws muaj Mohs hardness ntawm cuaj, yog pob tshab lossis semi pob tshab, thiab muaj lub ntsej muag ci ntsa iab.
Corundum yog tsim los ntawm qhov chaw sib cuag ntawm cov pob zeb metamorphic (xws li pob zeb siliceous), granulites, thiab lawv cov khaubncaws sab nraud povtseg. Nws muaj cov yam ntxwv xws li siab hardness, siab melting point, thiab corrosion kuj. Nws yog dav siv nyob rau hauv ntau yam kev lag luam teb raws li ib tug puas khoom thiab kuj muaj tej yam ornamental nqi.

image
Mineral Cheebtsam
Lub ntsiab tshuaj muaj pes tsawg leeg ntawm corundum yog Al2O3 (alumina). Qhov loj feem ntawm txhuas lub caij yog 53.2%, thiab qhov loj feem ntawm cov pa oxygen yog 46.8%. Muaj Cr3+, Ti4+, Fe3+, Fe2+, Mn2+, V3+, thiab lwm yam, lawv hloov Al3+ nrog qhov sib npaug lossis isovalent isomorphic isomers. Lub caij no, Al2O3 muaj ntau yam sib txawv, nrog - Al2O3 yog qhov ruaj khov tshaj plaws hauv qhov xwm txheej.
Lub cev muaj zog
Corundum yog nyob rau hauv daim ntawv ntawm tej thoob, kab, cones, thiab daim hlau, nrog ib tug nyuaj kev ntxhib los mos thiab feem ntau diagonal kab txaij nyob rau saum npoo. Ntshiab corundum yog xim tsis muaj xim lossis grey, daj grey, thiab nthuav tawm cov xim sib txawv vim muaj cov kab sib txawv, xws li dub rau hlau, liab rau chromium, xiav rau titanium, ntshav rau vanadium thiab chromium, thiab ntsuab rau hlau thiab chromium. iav luster. Tsis muaj cleavage; Feem ntau tshwm sim los ntawm kev tawg ntawm {0001} los yog {1011} vim yog kev tsim ntawm cov pob zeb ntxaib ntxaib lossis cov khoom zoo sib xws. Nyob rau hauv ntev thiab luv wavelength ultraviolet lub teeb, nws emits liab fluorescence, thaum cov uas muaj Fe ntsiab lus siab muaj zog fluorescence. Muaj Cr, nws nthuav tawm paj yeeb lossis txiv kab ntxwv daj fluorescence. Nws yog qhov ruaj khov ntawm chav tsev kub thiab kub hauv huab cua.
Cov xim cuam tshuam ntawm orthogonal polarizations ntawm corundum zoo ib yam li cov quartz, tab sis vim nws cov hardness siab, nws cov tuab feem ntau me ntsis loj dua li ntawm lwm cov ntxhia hauv tib zaj duab xis nyias. Yog li ntawd, cov xim cuam tshuam feem ntau ntau dua thawj - xaj dawb, thiab qee zaum tuaj yeem ncav cuag thib ob - xaj. Lub columnar txiav nto muaj qhov sib npaug ntawm kev tuag thiab cov cim tsis zoo elongation. Txawm li cas los xij, nws yuav tsum raug sau tseg tias rau corundum nrog lub phaj-zoo li tus cwj pwm, thaum cov yeeb yaj kiab nyias raug txiav rau ntawm lub dav hlau saum npoo, lub cim elongation ntawm ntu no yog qhov sib txawv, tab sis cov kev taw qhia elongation yog tib yam rau lub teeb qeeb. Feem ntau, qhov sib npaug {1011} ntxaib muaju tuaj yeem pom. Uniaxial crystals muaj qhov tsis zoo ntawm photosensitivity, tab sis qee zaum tshwm sim li biaxial crystals, nrog rau feem ntau me me optical axis kaum (txog li 58 degree). Txawm nyob rau hauv cov khoom siv dag zog ruby, qhov xwm txheej no tshwm sim, thiab cov kaum sab xis ntawm qhov chaw thiab cov npoo ntawm cov siv lead ua tsis sib npaug.
Cov cuab yeej tshuaj
Corundum yog cov kua qaub thiab alkali tiv taus, tab sis nyob rau hauv cov xwm txheej kub ntxhov thiab cov ntsiab lus alkali cov ntsiab lus, nws yuav raug cuam tshuam xws li Al2O3+2NaOH+3H2O=2NaAl (OH) 4, thiab cov tshuaj tiv thaiv yog cuam tshuam los ntawm qhov kub thiab txias. Noj 60% sodium hydroxide tov thiab cov tshuaj tiv thaiv lub sij hawm ntawm 6 teev raws li piv txwv, thaum kub nce ntawm 180℃mus rau 200 degree, lub dissolution tus nqi ntawm corundum nce los ntawm 12.5%. Txawm li cas los xij, raws li qhov ntsuas kub ntawm cov tshuaj tiv thaiv nce los ntawm 200℃mus rau 220 degree, qhov kev sib cais nce los ntawm 46%.