Dab tsi yog qhov cuam tshuam ntawm graphite zoo ntawm kev ua haujlwm ntawm magnesia carbon refractory cib?
Qhov zoo thiab cov txiaj ntsig ntawm magnesia carbon refractory cib yog ze ze rau qhov muaj graphite hauv magnesia carbon refractory cib, yog li qhov zoo ntawm graphite muaj feem cuam tshuam rau kev ua haujlwm ntawm magnesia carbon cib. Yog li dab tsi yog qhov cuam tshuam ntawm graphite ntawm magnesia refractory cib? Feem ntau tshwm sim hauv cov ntsiab lus hauv qab no:
Kev ua tau zoo ntawm refractory bricks
(1) Kev cuam tshuam ntawm graphite purity. Nrog rau qhov nce ntawm graphite purity, qhov yaig Performance index ntawm magnesia carbon bricks sharply txo thiab lub siab - kub flexural zog Performance index ho nce, tshwj xeeb tshaj yog thaum lub purity ntau dua 95%. Yog li ntawd, thaum siv graphite hauv magnesia carbon bricks, purity feem ntau yog siab dua 95%.
(2) Qhov cuam tshuam ntawm cov hmoov tshauv. Thaum SiO2 cov ntsiab lus nyob rau hauv graphite ntau tshaj 3%, qhov kev yaig Performance index ntawm magnesia carbon bricks nce ntau; Nyob rau tib lub sijhawm, impurities xws li SiO2 thiab Al2O3 kuj txo qhov hluav taws kub ntawm cov khoom, thiab cov ntsiab lus tshauv yuav cuam tshuam rau oxidation tsis kam ntawm cib. Yog li, nws yuav tsum tau hais tias cov ntsiab lus impurity ntawm graphite yuav tsum tsawg li tsawg tau.
(3) Cov nyhuv ntawm graphite oxidation kuj. Qhov kev txwv rau qhov corrosion ntawm cov khoom uas muaj cov khoom yog decarburization tus nqi. Yog li ntawd, oxidation tsis kam ntawm graphite muaj feem cuam tshuam rau corrosion kuj ntawm cov khoom. Qhov ntau ua tiav cov crystallization ntawm graphite, qhov me me ntawm thaj chaw tshwj xeeb, thiab qhov zoo dua qhov oxidation kuj. Yog li ntawd, graphite raw cov ntaub ntawv nrog ua tiav crystallization thiab zoo graphitization feem ntau yog xaiv rau zus tau tej cov magnesia carbon bricks.
(4) Kev cuam tshuam ntawm graphite particle loj thiab cov duab. Piv nrog rau lub ntiaj teb graphite, flake graphite tsis tsuas yog muaj siab purity, tab sis kuj muaj qhov tsis zoo crystallization. Yog li ntawd, cov khoom uas muaj cov khoom siv feem ntau siv flake graphite, thiab qhov loj thiab thinner lub flake particle loj, qhov zoo dua. Qhov me me me me ntawm graphite tuaj yeem txo qhov sib xyaw thiab molding zog, nrog rau oxidation tsis kam ntawm cov av nkos.
Dab tsi yog qhov cuam tshuam ntawm Graphite Zoo ntawm Kev Ua Haujlwm ntawm Magnesia Carbon Refractory Bricks?
Apr 20, 2026
Xa kev nug
Xov xwm tseeb
Tiv tauj peb
- Tel: +86-533-4188518
- Mob: +8613275332819
- E - Xa Ntawv: sdwenping@163.com
- Ntxiv: PAV 711, No.3, Yanhe Txoj kev, Boshan, Zibo, Shandong, Phiaj suav