Magnesia chrome cib yog tsim los ntawm kev siv siab -purity fused magnesia thiab hluavtaws magnesia zirconia ua cov ntaub ntawv tseem ceeb. Nws belongs rau alkaline refractory thiab haum rau alkali hlau thiab oxides. Sulfide muaj corrosion kuj zoo. Cov yam ntxwv zoo kawg li ntawm cov khoom yog: muaj zog alkali tsis kam, zoo slag kuj, muaj zog tev tsis kam, kub tsis kam thiab muaj zog hnav tsis kam. Magnesia chrome cib hloov siab -purity magnesia cib thiab magnesia chrome cib. Nws yog dav siv nyob rau hauv iav rauv, regenerator, cement kiln, steelmaking hluav taws xob rauv thiab lwm yam smelting furnaces.