1, Kev ntsuas ntsuas ntawm Graphitized Petroleum Coke
Yam khoom | Graphitized petroleum coke (graphitizing carburizer) |
Cov pa roj carbon monoxide% | Ntau dua lossis sib npaug rau 98.5 |
Sulfur% | Tsawg dua lossis sib npaug rau 0.05 |
Tshauv% | Tsawg dua los yog sib npaug rau 0.5 |
Volatile% | Tsawg dua los yog sib npaug rau 0.5 |
Cov dej noo% | Tsawg dua los yog sib npaug rau 0.5 |
Granularity hli | 1-5,1-10,5-10 |
2, Kev Paub Txog Graphitized Petroleum Coke
Graphitized petroleum coke yog ib hom roj av coke uas yog electrified thiab tom qab ntawd kho ntawm 3000 degree, Cov pa roj carbon molecular morphology ntawm roj av coke yog hloov los ntawm kev tsis sib xws rau hexagonal orderly arrangement.Qhov no roj av coke yuav zoo dua decomposed nyob rau hauv molten hlau, ib tug zoo carburant nyob rau hauv lub lag luam tam sim no, thiab yog ib tug indispensable metallurgical khoom nyob rau hauv steel-ua thiab foundry kev lag luam.
3, Cov yam ntxwv tseem ceeb ntawm cov khoom
1) Graphitization
2) Yooj yim rau nqus, qhov nqus yog 85-90%.
3) Tsawg impurities, txhim kho casting zoo thiab txo tus nqi
4, Ntim:25kg waterproof hnab + waterproof tonnage hnab
5, Chaw nres nkoj xa khoom:Qingdao / Tianjin
6, Cov khoom zoo:hmoov, columnar
7, Cov khoom ntim:
siv kev nyab xeeb, ruaj khov thiab noo noo-pov thawj packing haum rau kev thauj mus los hauv av thiab hiav txwv
8, Peb qhov kev pabcuam:
1) Muab cov lus qhia pub dawb rau cov neeg siv
2) Pub dawb rau cov neeg siv los muab cov lus piav qhia ntawm cov khoom siv
3) Dawb rau cov neeg siv los muab cov khoom tsim qauv tsim qauv
4) Dawb rau cov neeg siv los muab cov qauv, rau cov neeg siv kev sim
9, Peb qhov zoo:
1) Kev tshaj lij, nrog ntau tshaj 20 xyoo ntawm kev tsim khoom thiab kev lag luam, muaj zog sib pauv thiab kev pabcuam
2) Peb muaj peb tus kheej Refractory cov khoom tsim kev koom tes Hoobkas
3) Peb muaj peb tus kheej Graphite Electrode khoom tsim kev koom tes Hoobkas
10.Cov lus pom zoo ntawm cov khoom siv tau zoo, cov khoom tau raug xa tawm mus rau Australia, Oman, Mexico
11.Peb yog cov kws tshaj lij kev lag luam, uas tuaj yeem muab cov neeg siv khoom siv khoom siv dawb, siv thiab lwm yam teeb meem.
Koj puas xav nrhiav tus kws tshaj lij ntawm Graphitized Petroleum Coke khoom?
Koj puas xav nrhiav tus neeg muag khoom ruaj khov thiab ntseeg tau?
Tom qab ntawd thov hu rau peb
Hu rau kuv: Email: wp@cnjingganrefractory.com/sdwenping@163.com
TEL: 86-0533-4188518 / Fax: 86-0533-4188518
Rose: +86-13275332819(wechat/whatsapp tus xov tooj)
Cim npe nrov: Graphitized Carburant, Suav teb, manufacturers, lwm tus neeg, Hoobkas, siv, khoom