Castable rau hauv ob sab phlu ntawm aluminium melting reverberatory rauv kuj hu ua non nodulation castable. Nws yog tshwj xeeb yog siv rau txhuas smelting reverberatory rauv. Nws tsis muaj aluminium stick thiab nodulation nyob rau hauv tus txheej txheem ntawm kev siv. Nws muaj qhov kub thiab txias tsis kam thiab corrosion kuj ntawm cov kua txhuas. Lub ntsiab siv lead ua theem ntawm cov khoom yog mullite, uas yog thawj-chav tsim nyog cov khoom.
Xa kev nug
Tsham tam sim no
Hauj lwm lawm

1, Kev piav qhia ntawm Lining castable rau molten aluminium reverberatory rauv
Cov khoom yog ib tug siab purity mullite-raws li tsawg cement castable siv nyob rau hauv reverberatory rauv lub cev qhov chaw. Cov khoom muaj zoo ntim stability, anti-aluminium penetration muaj peev xwm, zoo compactness thiab anti-spalling kev ua tau zoo. Cov khoom muaj tsawg SIO2 thiab FeO3, uas tiv thaiv kev loj hlob ntawm corundum qog.

2, Index of Lining castable for molten aluminium reverberatory cub

Yam khoom

JAF-70

Al2O3%

>65

Grain loj mm

0-6

Ua haujlwm kub degree

1350

Qhov ntom ntom g / cm3

2.40

Compression zog Mpa

110℃      >50

1200℃    >65

1350℃     >80

Kab hloov tus nqi 1100 degree%

±0.20


3, Cov yam ntxwv tseem ceeb ntawm castable rau sab hauv txheej ntawm molten aluminium reverberatory rauv

1) Cov khoom muaj ob peb impurities, feem ntau yog cov ntsiab lus qis ntawm SO2 thiab Fe2O3, uas zoo tiv thaiv kev tsim ntawm corundum qog.

2) Cov khoom lag luam muaj kev ua haujlwm zoo los tiv thaiv tev, thiab nws tsis yooj yim rau poob ntawm slag thaum siv kub.

3) Lub shrinkage tus nqi ntawm cov khoom yog me me, thiab kev ncaj ncees thiab compactness ntawm masonry qauv yog tswj.

4, Cov ntawv sau ntxiv:

1) Cov khoom yuav tsum tau premixed uniformly ua ntej siv, thiab txoj kev tsim yog pouring.
2) Cov khoom tau ntim rau hauv lub hnab tsis muaj dej, thiab lub sijhawm cia yog 6 lub hlis.

5.Cov lus pom zoo ntawm cov khoom siv tau zoo, cov khoom tau raug xa tawm mus rau Australia, Oman, Tebchaws Meskas

6.Cov chaw tsim khoom yog cov chaw tsim khoom lag luam thiab tuaj yeem muab cov khoom lag luam ua tiav cov ntaub ntawv ntsuam xyuas lossis cov ntaub ntawv xeem thib peb.



Koj puas xav nrhiav tus kws tshaj lij ntawm cov khoom castable?


Koj puas xav nrhiav tus neeg muag khoom ruaj khov thiab ntseeg tau?


Tom qab ntawd thov hu rau peb



Hu rau kuv:

Email: wp@cnjingganrefractory.com/sdwenping@163.com

TEL: 86-0533-4188518 / Fax: 86-0533-4188518

Rose: +86-13275332819(wechat/whatsapp tus xov tooj)


Cim npe nrov: Sab hauv Castable Rau Molten Aluminium Reverberatory Rauv, Tuam Tshoj, tuam ntxhab, lwm tus muag khoom, Hoobkas, siv, khoom

Xa kev nug
Tiv tauj peb
  • Tel: +86-533-4188518
  • Mob: +8613275332819
  • E - Xa Ntawv: sdwenping@163.com
  • Ntxiv: PAV 711, No.3, Yanhe Txoj kev, Boshan, Zibo, Shandong, Phiaj suav

(0/10)

clearall