1, Nqe lus piav txog Corundum Castable rau Cov Rauv Hluav Taws Xob Sab saum toj:
Corundum Castable rau Cov Rauv Hluav Taws Xob Sab saum toj siv fused dawb corundum xuab zeb ua cov khoom siv tseem ceeb, ntxiv me me ntawm cov khoom siv tshwj xeeb thiab siv cov ntshiab calcium aluminate cement ua cov ntawv. Cov khoom muaj lub zog siab thiab ntom ntom siab tom qab ziab hauv qhov txheej txheem ntawm kev siv, Corundum Castable rau Cov Rauv Hluav Taws Xob Sab saum toj muaj cov txheej txheem corundum ua lub hauv paus tseem ceeb. Nws muaj kev tiv thaiv corrosion zoo heev, cuam tshuam tiv taus thiab siv tau zoo.
2, Index ntawm Corundum Castable rau Cov Rauv Hluav Taws Xob Sab saum toj:
| Qauv | JDR-80 | |
| Yam khoom | ||
Muaj pes tsawg leeg | Al2O3 | ≥80 |
Cr2O3 | ---- | |
CaO | ≤2.0 | |
Tej ntom ntom g/cm³ | 110℃*24h | ≥2.75 |
1500℃*3h | ≥2.70 | |
Crushing zog MPa | 110℃*24h | ≥80 |
1500℃*3h | ≥100 | |
Hloov pauv tus nqi% | 1500℃*3h | ±0.5 |
3, Cov khoom lag luam tseem ceeb:
1) Lub zog muaj zog, ruaj khov ntawm cov kab hluav taws xob ntawm qhov kub
2) High ceev, Integral hauv ob sab phlu muaj muaj zog ua hauj slag yaig thiab allergic
3) Muaj zog tiv taus rau cov khoom me me, plua plav thiab pa roj av
4) Tsis kam mus rau cov khoom siv coj los kua muag
5) tsis cuam tshuam los ntawm kev txo cov roj cua xws li H2 thiab CO
4, Daim Ntawv Thov ntawmCorundum Castable rau Cov Rauv Hluav Taws Xob Sab saum toj
1) Ua haujlwm kub ntawm cov khoom yog 1600 ℃ -1700 ℃
2) Hluav Taws Xob Hluav Taws Xob
3) LF Rauv Npog
4) Petrochemical Catalytic Cracking Reactor
5) Boiler Kub Kub Coj Ua Haujlwm Thaj Tsam
5, Txoj kev tsim kho:
nchuav moulding lossis tsim ntawm qhov chaw mus rau hauv cov tsev prefabricated
Ntim: Dej tsis muaj dej, pov thawj cov hnab ntawv kraft, khaws cia hauv ib puag ncig qhuav ntau dua 6 lub hlis
6.Qhov zoo tswv yim ntawm kev siv cov khoom lag luam, cov khoom tau raug xa tawm mus rau Tebchaws Meskas, Kenya, Mexico
7.Qhov chaw tsim khoom yog cov chaw tsim khoom lag luam thiab tuaj yeem muab cov ntaub ntawv ntsuas ntsuas khoom tiav lossis cov ntawv xeem thib peb.
Koj puas xav nrhiav tus kws tshaj lij ntawm cov khoom lag luam miv?
Koj puas xav nrhiav tus neeg muag khoom ruaj khov thiab ntseeg tau?
Tom qab ntawv thov hu rau peb
Hu rau kuv: Email: wp@cnjingganrefractory.com/sdwenping@163.com
TEL: 86-0533-4188518 / FAX: 86-0533-4188518
Rose: +86-13275332819 (wechat/tus lej whatsapp)
Cim npe nrov: corundum castable rau hluav taws xob rauv sab saum toj, Tuam Tshoj, tuam ntxhab, cov chaw muag khoom, lub Hoobkas, siv, khoom