Kho Refractory Rau Hluav Taws Xob Hluav Taws Xob tseem hu ua ramming khoom rau hluav taws xob rauv hauv qab lossis ramming khoom rau hluav taws xob rauv txoj kab nqes. Nws cov khoom tseem ceeb yog MgO, CaO thiab Fe2O3, nrog rau siab adhesion tus nqi, zoo hnav tsis kam thiab corrosion kuj ntawm molten steel, thiab ntev kev pab cuam lub neej. Nws yog feem ntau siv nyob rau hauv high-power thiab ultra-high-power hluav taws xob furnaces. Thawj cov khoom tsim nyog, hom TRR.
Xa kev nug
Tsham tam sim no
Hauj lwm lawm

1, Kev ua haujlwm tseem ceeb ntawm Kho Refractory Rau Hluav Taws Xob

Yam khoom

Chav tsev

Tus nqi

MgO

feem pua

>80

Al2O3

feem pua

0.5

Fe2O 3

feem pua

5.5-6.0

CaO

feem pua

11-12

SIB 2

feem pua

1.5

Qhov ntom

G / cm3

>3.0

Kev pabcuam kub

degree

1700

Particle loj

mm

0-6

Compression zog

Mpa

110 degree ~ 25

1300 degree ~ 35

1500 degree ~ 40

Flexural zog

Mpa

110 degree ~ 10

1300 degree ~ 18

1500 degree ~ 20

2, Product Description ofKho Refractory Rau Hluav Taws Xob

Kho Refractory Rau Hluav Taws XobNws muaj qhov zoo ntawm qhov kub thiab txias lub zog, kev ua tau zoo tag nrho tom qab kev tsim kho, siab adhesion tus nqi, tsis tshua muaj rebound tus nqi, tsis kam mus rau molten steel scouring thiab yaig, zoo heev thermal shock kuj, zoo sintering kev ua tau zoo, yooj yim rau tsim nyuaj ntom txheej thiab ntev kev pab cuam lub neej, Cov khoom tsim nyog rau kev ua hauj lwm hauv ob sab phlu ntawm lub cub tawg hauv qab thiab txoj kab nqes ntawm lub zog siab thiab ultra-siab zog hluav taws xob rauv

3, Khoom duab thiab siv daim duab

image

4. Cov yam ntxwv tseem ceeb ntawm cov khoom

1) Kev ua tau zoo sintering, yooj yim los tsim cov txheej txheej nyuaj, yog li tiv taus molten hlau yaig thiab yaig

2) Zoo adhesion, tsim kom tiav compact tag nrho, uas yog, siab structural zog ntawm kub kub

3) Cov thermal shock kuj zoo heev, tsis yooj yim rau tev tawm, lub neej ua haujlwm ntev

4) Hauv qab ntawm lub tshuab hluav taws xob, qhov ua haujlwm hauv ob sab phlu ntawm lub cub tawg yog siv tau zoo

5. Daim ntawv thov hom: tamping lossis tshuaj tsuag kho

6. Cia: cov khoom muaj MgO thiab CaO, uas yooj yim rau kev cuam tshuam los ntawm dampness thiab txo qhov kev ua tau zoo ntawm cov khoom. Cov khoom yuav tsum tau muab kaw, tsis muaj dej noo thiab ntim nrog lub teeb tsis muaj dej. Cov khoom yuav tsum tau muab cia rau hauv ib qho chaw ventilated thiab qhuav. Nws yog qhov zoo dua los thov cov khoom lag luam hauv lub sijhawm luv luv kom ntseeg tau tias cov khoom siv tau zoo

7, Cov lus pom zoo ntawm cov khoom siv tau zoo, cov khoom tau raug xa tawm mus rau Kaus Lim Qab Teb, Nyiv, Pakistan

8, Peb yog cov kws tshaj lij kev lag luam, uas tuaj yeem muab cov neeg siv khoom siv khoom siv dawb, siv thiab lwm yam teeb meem




Koj puas xav nrhiav tus kws tshaj lij ntawm Kev Kho Refractory Rau Hluav Taws Xob Hluav Taws Xob


Koj puas xav nrhiav tus neeg muag khoom ruaj khov thiab ntseeg tau?


Tom qab ntawd thov hu rau peb



Hu rau kuv:

Email: wp@cnjingganrefractory.com/sdwenping@163.com

TEL: 86-0533-4188518 / Fax: 86-0533-4188518

Rose: ntxiv rau 86-13275332819(wechat/whatsapp tooj)


Cim npe nrov: kho refractory rau hluav taws xob rauv, Suav teb, manufacturers, lwm tus neeg, Hoobkas, siv, khoom

Xa kev nug
Tiv tauj peb
  • Tel: +86-533-4188518
  • Mob: +8613275332819
  • E - Xa Ntawv: sdwenping@163.com
  • Ntxiv: PAV 711, No.3, Yanhe Txoj kev, Boshan, Zibo, Shandong, Phiaj suav

(0/10)

clearall