1, Cov yam ntxwv tshwj xeeb
1) Cov khoom siv tau ruaj khov, tsis yooj yim rau deform, ruaj khov
2) Lub qhov ntom ntom yog cov khaub ncaws hnav thiab muaj lub suab zoo insulation nyhuv
3) Cov tshuaj tiv thaiv dej, noo noo-pov thawj, tsis tshua muaj dej nqus, tiv thaiv corrosion
2, Specification
Thickness: 4,6,8,10mm Pob qhov taub: 6,8,10,12mm
Dav: 600,1220mm Ntev: 1200,2440,3000mm

3, Main Performance Parameters
Yam khoom | UNIT | TECHNCIAL INDEX |
Qhov ntom | g/cm3 | >1.2 |
Thermal conductivity | w/m.k | Tsawg dua lossis sib npaug rau 0.30 |
Kev nqus dej | % | Tsawg dua los yog sib npaug li 45 |
Tus nqi o | % | Tsawg dua lossis sib npaug rau 0.25 |
Fireproofing kev ua tau zoo | A qib | |
Flexural zog | Mpa | Ntau dua lossis sib npaug li 12 |
Kev cuam tshuam lub zog | Kj/m2 | Ntau dua lossis sib npaug rau 1.8 |
4, Zoo heev nta:
1) Zoo noo noo tsis kam, tsis muaj expansion lossis deformation
2) Nws yog hluav taws-retardant thiab yuav tsis tsim cov pa phem
3) Tsis muaj asbestos, tsis muaj tshuaj lom, tsis muaj hluav taws xob
4) Lub zog loj, lub teeb yuag
5) Thaum tshav kub kub rwb thaiv tsev, suab nqus, txo suab nrov
6) anti-aging, mildew proofing thiab npauj pov thawj.
5, Peb lub tuam txhab cog lus rau cov neeg siv khoom: muab cov kev sib pauv thiab kev pabcuam pub dawb nrog cov neeg siv khoom, thiab muab cov qauv rau cov neeg siv khoom dawb yam tsis muaj nqi coj mus kuaj.
6, Kev Ua tiav tau tsim: Peb lub tuam txhab yav dhau los tau xa 160 tons rau Pakistan.
Koj puas xav nrhiav tus kws tshaj lij ntawm Perforated Calcium Silicate Boards?
Koj puas xav nrhiav tus neeg muag khoom ruaj khov thiab ntseeg tau?
Tom qab ntawd thov hu rau peb
Hu rau kuv:
Email: wp@cnjingganrefractory.com/sdwenping@163.com
TEL: 86-0533-4188518 / Fax: 86-0533-4188518
Rose: +86-13275332819(wechat/whatsapp tus xov tooj)
Cim npe nrov: perforated calcium silicate board, Tuam Tshoj, manufacturers, lwm tus neeg, Hoobkas, siv, khoom