Kev taw qhia luv luv: Xonotlite Composite Cib yog cov khoom siv tsis muaj zog, uas yog ua los ntawm cov khoom siv siliceous thiab cov khoom siv calcareous. Cov khoom lag luam sib npaug sib npaug nrog ntau tus micron qib pores, thiab cov porosity ncav cuag 85-90%. Nws muaj kev ua haujlwm zoo ntawm rwb thaiv tsev. Cov khoom tsis muaj asbestos thiab lwm yam teeb meem, tsis mildew, lwj, siv tau zoo, lub neej ntev
Xa kev nug
Tsham tam sim no
Hauj lwm lawm

1, Product Performance Parameters

Yam khoom

UNIT

FSC-300

FSC-400

FSC-220

FSC-550

Ua haujlwm kub

degree

1000

1000

1000

1200

Qhov ntom

Kg / m3

300±10

400±10

220±10

550±10

Compressive zog

Mpa

Ntau dua lossis sib npaug li 1.5

Ntau dua lossis sib npaug rau 2.0

Ntau dua lossis sib npaug rau 0.33

Ntau dua lossis sib npaug rau 0.6

Linear shrinkage

900 degree * 3h

%

Tsawg dua los yog sib npaug rau 1.0

Tsawg dua los yog sib npaug rau 1.0

1000 degree * 3h

Tsawg dua lossis sib npaug rau 2.0

1100 degree * 3h

Tsawg dua los yog sib npaug rau 3.0

Thermal conductivity

900 degree

W/m.k

Tsawg dua lossis sib npaug rau 0.11

Tsawg dua lossis sib npaug rau 0.13

700 degree

Tsawg dua lossis sib npaug rau 0.09

1100 degree

Tsawg dua lossis sib npaug rau 0.14

Cov ntawv thov tseem ceeb


Electrolytic aluminium kev lag luam

Electrolytic aluminium kev lag luam

Kev lag luam cement

Kev lag luam cement

2~AL~OB`9$O1AX0__(~ZGL0


2, Cov yam ntxwv ntawm Xonotlite Composite Board:

1) Me me thermal conductivity, zoo thermal rwb thaiv tsev nyhuv

2) Qhov kub thiab txias shrinkage yog me me thiab loj yog ruaj khov

3) Qhov ceev me me, lub teeb yuag, muaj peev xwm ua kom sov tsawg

4) ruaj khov lub cev thiab tshuaj lom neeg, siv tau zoo

3, Daim ntawv thov: nws yog tsuas yog siv rau thermal rwb thaiv tsev txheej ntawm electrolytic aluminium kev lag luam, cement kev lag luam thiab lwm yam lag luam

4, Peb lub tuam txhab cog lus rau cov neeg siv khoom: los muab kev sib pauv thiab kev pabcuam pub dawb nrog cov neeg siv khoom, thiab muab cov qauv rau cov neeg siv khoom dawb yam tsis muaj nqi coj mus kuaj.

5, Kev Ua tiav tau tsim: Peb lub tuam txhab yav dhau los tau xa 90 tons rau Oman.




Koj puas xav nrhiav tus kws tshaj lij ntawm Xonotlite Composite Board?


Koj puas xav nrhiav tus neeg muag khoom ruaj khov thiab ntseeg tau?


Tom qab ntawd thov hu rau peb


Hu rau kuv:

Email: wp@cnjingganrefractory.com/sdwenping@163.com

TEL: 86-0533-4188518 / Fax: 86-0533-4188518

Rose: +86-13275332819(wechat/whatsapp tus xov tooj)


Cim npe nrov: Xonotlite Composite Board, Suav teb, manufacturers, lwm tus neeg, Hoobkas, siv, khoom

Xa kev nug
Tiv tauj peb
  • Tel: +86-533-4188518
  • Mob: +8613275332819
  • E - Xa Ntawv: sdwenping@163.com
  • Ntxiv: PAV 711, No.3, Yanhe Txoj kev, Boshan, Zibo, Shandong, Phiaj suav

(0/10)

clearall