Lub npe tag nrho ntawm cov khoom yog siab-purity fused quartz ceramic crucible, nrog SiO2 cov ntsiab lus ≥ 99.9%. Cov khoom lag luam yog ceramic crucible ua los ntawm high-purity fused quartz, Nws cov duab yog tsuas yog square thiab cylindrical. Cov khoom siv square yog siv rau kev sib xyaw ntawm polysilicon, thiab cov khoom sib luag yog siv rau kev kos duab ntawm monocrystalline silicon. Cov khoom lag luam yog siv ntawm 1450 ℃, nrog lub siab qhov loj me, tsis muaj qhov deformation ntawm qhov kub, qhov zoo thermal poob siab thiab tshuaj lom neeg tsis kam.
Xa kev nug
Tsham tam sim no
Hauj lwm lawm

1, Tshuaj lom neeg muaj pes tsawg leeg ntawm cov khoom

Qib

Hnub ci qib

Electronics qib

Khoom cua

Al

18

7.5

20

Fe

0.2

0.2

27

Ca

0.6

0.5

23

Na

1.1

0.3

8

K

0.9

0.1

1

Li

0.7

0.2

1

Cov Ti

1.1

1.4

25

Cr

0.05

0.05

2

N

0.05

0.05

1

Meb

0.05

0.05

9

B

0.08

0.04

10

P

0.05

0.02

10

OH

50

50

50

2, Kev Qhia Tshwj Xeeb ntawm Quatz ceramic crucible

Hom

Tawm taub

Qhov siab

hli

Phab ntsa thicknesss1

hli

Phab ntsa tuab2

hli

Phab ntsa thicknesss3

hli

Radius1

hli

Ntse2

hli

10’’

254±2

178±3

7.0±2

7.0±2

7.0±2

305

70

12’’

305±2

228±3

8.0±2

8.0±2

8.0±2

305

80

14’’

355±2

254±3

9.0±2

9.0±2

9.0±2

400

90

16’’

404±2

305±3

9.5±2

9.5±2

9.5±2

400

90

18’’

457±2

355±3

9.5±2

9.5±2

10.0±2

500

120

20’’

508±2

381±3

10.0±3

10.0±2

11.0±2

510

120

22’’

558±5

381±3

10.0±3

10.0±3

11.0±2

558

130

24’’

610±5

381±3

11.0±3

11.0±3

12.0±2

610

130

3, Daim Ntawv Thov: iav ua tob, kev lag luam nws yog xim hlau, kev lag luam hluav taws xob, kev lag luam chemical, kev lag luam aerospace

4, Lwm tus: cov khoom yog translucent dawb, zoo nkauj thiab zoo nkauj. Nws yog tsuas yog tsim los ntawm arc txoj kev, thiab txheej sab hauv yog txheej nrog 0.6-2mm barium hydroxide txheej los xyuas kom meej thiab txuas ntxiv siv cov nyhuv ntawm cov khoom

5, Kev ntim: carton, shatter pov thawj thiab noo noo-ntawv pov thawj

6, Cov lus teb zoo ntawm cov khoom siv tau zoo, cov khoom lag luam tau xa tawm mus rau Kaus Lim Qab Teb, Russia, Pakistan

7, Peb yog cov kws tshaj lij kev lag luam, uas tuaj yeem muab cov qhua tuaj yeem siv cov khoom lag luam pub dawb, siv thiab lwm yam teeb meem






Koj puas xav nrhiav tus kws tshaj lij ntawm cov khoom lag luam refractory?


Koj puas xav nrhiav tus kws tshaj tawm cov khoom hluav taws xob graphite?


Koj puas xav nrhiav tus neeg xa khoom kom ruaj khov thiab lees paub?


Tom qab ntawd cia' s kev sib cuag nrog jinggan tuam txhab




Hu rau kuv:

Email: wp@cnjingganrefractory.com/sdwenping@163.com

TEL: 86-0533-4188518 / FAX: 86-0533-4188518

Rose: +86-13275332819 (wechat / whatsapp tooj)


Cim npe nrov: quartz ceramic crucible, Tuam Tshoj, tuam ntxhab, cov chaw muag khoom, lub Hoobkas, siv, vaj tse

Xa kev nug
Tiv tauj peb
  • Tel: +86-533-4188518
  • Mob: +8613275332819
  • E - Xa Ntawv: sdwenping@163.com
  • Ntxiv: PAV 711, No.3, Yanhe Txoj kev, Boshan, Zibo, Shandong, Phiaj suav

(0/10)

clearall