Seamless Yeeb Nkab Rau Lub Hom Phiaj

Seamless Yeeb Nkab Rau Lub Hom Phiaj

cov yeeb nkab tsis sib xyaw ua ke tau muab faib ua kub dov thiab txias txias, suav nrog cov txheej txheem cov yeeb nkab steel, lub npe muaj Q195 , Q235 A, B, C, D, Q275 thiab ntxiv rau, Tsawg alloy siab zog muaj zog cov qauv hlau yeeb nkab, hom muaj Q345 A, B, C, Q460 C. Cov yeeb nkab steel muaj lub zog siab, ua haujlwm tau zoo, kev pab lub neej ntev thiab kev thov dav. Nws tau siv dav hauv cov choj, nkoj, rhaub dej, tsheb thiab cov tsev tsim khoom tseem ceeb. Cov khoom lag luam tuaj yeem ua rau hauv daim hlau, cov duab, cov yeeb nkab tsis sib haum, thiab lwm yam.
Xa kev nug
Tsham tam sim no
Hauj lwm lawm

1, Khoom ua haujlwm tsis:

Hom

Q345 C qib

20#

C %

≤0.20

0.17-0.23

SI %

≤0.55

0.15-0.40

Mn %

≤1.70

0.35-0.65

S %

≤0.035

≤0.035

P %

≤0.035

≤0.035

V %

0.02-0.15


Nb %

0.015-0.060


AI

≥0.015


Ti

0.02-0.20


Cr


≤0.25

Nws


≤0.25

Cu


≤0.25

qhov kub thiab txias ℃


-20-425

tensile lub zog Mpa

≥490

≥420

tawm dag zog Mpa

160-350

≥250

2, Cov lus qhia tshwj xeeb: phab ntsa tuab: 2.5-200mm , 89*5,89*5.5,89*6,89*7, ntev ≥500mm, thiab ntxiv rau ...

3, Tus lej tus lej: GB8162-2008, sib npaug rau ASTM A53

4, Cov Lus Qhia: Nyob zoo cov neeg siv, vim muaj ntau tus qauv thiab qhov ntau ntawm cov khoom, thaum koj xav tau lawv, thov qhia meej meej ua ntej cov qauv khoom, qhov loj me, kev ntsuas ua tau zoo, kev siv, kev yuav khoom ntau, thiab lwm yam, yog li kuv tuaj yeem muab rau koj tus nqi tshwj xeeb rau cov khoom raug

5, Peb lub tuam txhab xa tawm cov khoom zoo li no txhua xyoo puag ncig, nrog cov khoom siv ntau. Txais tos kom sib tham.

6.Qhov zoo tswv yim ntawm kev siv cov khoom lag luam, cov khoom tau raug xa tawm mus rau Kaus Lim Qab Teb, Oman, Morocco

7.Peb yog tus muab khoom tshaj lij, leej twg tuaj yeem muab cov neeg siv khoom siv thev naus laus zis dawb, siv thiab lwm yam teeb meem.



Koj puas xav nrhiav tus kws tshaj lij ntawm Seamless Yeeb Nkab cov khoom lag luam?

Koj puas xav nrhiav tus neeg muag khoom ruaj khov thiab ntseeg tau?

Tom qab ntawv thov hu rau peb

Tiv tauj kuv:

Email: wp@cnjingganrefractory.com/sdwenping@163.com

TEL: 86-0533-4188518 / FAX: 86-0533-4188518

Rose: +86-13275332819 (wechat/tus lej whatsapp)



Cim npe nrov: seamless yeeb nkab rau kev teeb tsa lub hom phiaj, Tuam Tshoj, tuam ntxhab, cov chaw muag khoom, lub Hoobkas, siv, khoom

Xa kev nug
Tiv tauj peb
  • Tel: +86-533-4188518
  • Mob: +8613275332819
  • E - Xa Ntawv: sdwenping@163.com
  • Ntxiv: PAV 711, No.3, Yanhe Txoj kev, Boshan, Zibo, Shandong, Phiaj suav

(0/10)

clearall