1, Kev piav qhia: Lub ntsiab ntxhia theem ntawm cordierite honeycomb ceramics yog cordierite mullite theem. Yog li ntawd, nws tseem hu ua cordierite mullite honeycomb ceramics. Nws muaj zoo heev quenching thiab cua sov tsis kam thiab corrosion kuj. Nws tuaj yeem txo qhov emission ntawm CO2 thiab nitrogen oxides thiab purify lub flue roj.
Cov khoom lag luam yog tsim los ntawm hluavtaws cordierite thiab cov nplaum los ntawm cov txheej txheem molding thiab kub kub firing. Lawv feem ntau yog siv rau hauv lub tsheb tso pa catalytic purification, industrial kiln tshem tawm plua plav thiab tshav kub cia, roj av catalytic cracking thiab lwm yam lag luam.
Cov khoom muaj tsawg ntom ntom, tsawg coefficient ntawm thermal expansion, zoo thermal ruaj khov thiab cuam tshuam tsis kam. Nws yog dav siv nyob rau hauv lub tshav pob ntawm kev txo lub tsheb pa emissions. Yuav ua li cas txo cov coefficient ntawm thermal expansion dua, txo qhov kev puas tsuaj ntawm thermal kev nyuaj siab, thiab txhim kho cov thermal shock kuj ntawm cov khoom yog tus yuam sij los txhim kho lub neej ntawm cordierite honeycomb ceramics tam sim no.
2, Main technical parameters ntawm cov khoom
Yam khoom | UNIT | TECHNCIAL INDEX |
SIB 2 | % | 50-54 |
Al2O3 | % | 28-34 |
MgO | % | 11-14 |
Fe2O 3 | % | <1 |
TSO 2 | % | <1 |
Tshwj xeeb kub muaj peev xwm | kj/kg | 900-1100 |
Tshwj xeeb lub ntiajteb txawj nqus | kg/m3 | 1.6-1.9 |
Coefficient ntawm tshav kub conductivity | w/m.k | 1.2-1.8 |
Acid kuj | % | Ntau dua lossis sib npaug li 95 |
Kev nqus dej | % | 17-22 |
Kev pabcuam kub | degree | 1200 |
2, Khoom specifications thiab lub cev tsis muaj Cordierite Honeycomb Ceramic
Specification
mm | Tus naj npawb ntawm qhov | Phab ntsa thickness
mm | Qhov chaw tshwj xeeb
m2/m3 | Voidage
% | B.D
kg/m3 |
150*150*300 | 60*60 | 0.5 | 1315 | 70 | 680 |
150*150*300 | 50*50 | 0.7 | 1050 | 58 | 680 |
150*150*300 | 40*40 | 0.7 | 883 | 65 | 518 |
150*150*300 | 25*25 | 1.0 | 573 | 67 | 502 |
3, Nta thiab kev ua haujlwm ntawm Cordierite Honeycomb Ceramic:
1) Nws tuaj yeem rov qab tau cov hluav taws kub ntawm cov pa hluav taws xob zoo, paub lub zog txuag, txhim kho thermal efficiency ntawm cov khoom siv thermal thiab txo CO2 emissions
2) Qhov kub ntawm qhov cub tawg yog qhov sib xws, thiab NO x emission nyob rau hauv cov roj flue tuaj yeem txo qis dua 40%
3) Ua kom qhov kub thiab txias hauv lub cub tawg thiab txhim kho cov cua sov hloov hauv qhov cub
4) Lub zog txuag hluav taws xob muaj peev xwm thiab tshuaj tiv thaiv corrosion
5) Muaj peev xwm tshwj xeeb kub thiab zoo thermal conductivity
4, Daim ntawv thov teb: petrochemical kev lag luam, steel cog, khib nyiab incinerator, khib nyiab kho rauv, fais fab nroj tsuag, boiler, thiab lwm yam
5, Peb lub tuam txhab cog lus rau cov neeg siv khoom: los muab kev sib pauv thiab kev pabcuam pub dawb nrog cov neeg siv khoom, thiab muab cov qauv rau cov neeg siv khoom dawb yam tsis muaj nqi coj mus kuaj.
6, Kev Ua tiav tau tsim: Peb lub tuam txhab yav dhau los tau xa 80 tons rau Canada.
Koj puas xav nrhiav tus kws tshaj lij ntawm Cordierite Honeycomb Ceramic khoom?
Koj puas xav nrhiav tus neeg muag khoom ruaj khov thiab ntseeg tau?
Tom qab ntawd thov hu rau peb
Hu rau kuv:
Email: wp@cnjingganrefractory.com/sdwenping@163.com