Kev piav qhia ntawm Electrode Paste
1, Siv cov ntaub ntawv raw: calcined anthracite, calcined petroleum coke, kua asphalt, graphite hmoov, antioxidant additives, thiab lwm yam.
2, Cov txheej txheem yooj yim ntawm cov khoom tsim: raw khoom crushing, nruab nrab crushing, sib tsoo, cov khoom xyaw, cua sov, kneading, shaping, txias, ntim.
3, Cov Khoom Muag: Cov khob cij thaiv, Trapezoid thaiv.
4, Cov yam ntxwv: Kub kub tsis kam, me me coefficient ntawm thermal expansion, me me coefficient ntawm tsis kam, thiaj li yuav txo tau ntawm hluav taws xob. Tsawg porosity los txo cov oxidation ntawm cov khoom nyob rau hauv cua sov thiab siab mechanical zog.
5, Daim ntawv thov: Ferroalloy rauv, calcium, carbide rauv thiab lwm yam khoom siv smelting.
6, Index ntawm Electrode Paste
Yam khoom | JH-80 |
Cov pa roj carbon monoxide% | >80 |
Tshauv% | <7 |
Volatiles% | 11-15 |
Compression zog Mpa | >20 |
Resistivity μΩ•m | 65-75 |
PEB g/cm3 | >1.40 |
Cov ntsiab lus dej% | <0.5 |
Extensibility% | 5-20 |
7, Kev siv cov khoom siv
Electrode paste, tseem hu ua self-baking electrode, nws tso siab rau cov cua sov hauv lub qhov cub submerged arc kom tiav cov roasting. Yog li ntawd, qhov sib piv ntawm kev noj cov khoom noj nrog tus nqi ci yog tus yuam sij rau kev siv cov khoom siv. Kev ua haujlwm sintering ntawm electrode muab tshuaj yog qhov zoo. Yog tias kev ua haujlwm thev naus laus zis thiab ib puag ncig ntawm lub Hoobkas raug siv kom tsim nyog thiab tsim nyog, kev siv cov khoom siv yuav zoo dua.
Ob qhov kev txhawj xeeb tshaj plaws ntawm daim ntawv thov lub Hoobkas yog qhov muag muag thiab tawv tawg ntawm electrode paste thaum nws siv. Mos so yog vim tsis txaus cua sov ntawm cov khoom, uas ua rau tsawg sintering ceev tshaj li noj ceev, poob sai heev, cov khoom tsis siab sintered tsis tuaj yeem tiv taus qhov qis ntawm cov khoom nro thiab lateral cuam tshuam, ua rau tawg. Lub zog tawg yog tshwm sim los ntawm lub zog tsis txaus ntawm cov khoom tom qab sintering.
Qhov tshwm sim ntawm ob qhov teeb meem no muaj feem xyuam nrog cov khoom ua tau zoo ntawm cov chaw tsim khoom thiab kev ua haujlwm zoo ntawm lub Hoobkas. Tsuav yog cov chaw tsim khoom nruj me ntsis xaiv cov khoom siv raw rau kev faib ua feem, xaiv cov khoom siv tsis tu ncua ob-axis kneading lauj kaub nrog ntau tshaj 2000 L, thiab tuav lub kneading ceev thiab lub sij hawm zoo, Tsis tas li ntawd, tsim nyog xaiv qhov muag muag (90 degree) ntawm asphalt binder thiab tus nqi ntawm kev siv thiab roasting ceev ntawm cov khoom, nruj tswj ntawm cov yam tseem ceeb ntawm ntau lawm, kev ua tau zoo ntawm cov khoom electrode muab tshuaj txhuam yuav tsim nyog kiag li.
9.Peb yog cov kws tshaj lij kev lag luam, uas tuaj yeem muab cov neeg siv khoom siv khoom siv dawb, siv thiab lwm yam teeb meem.
10, Peb lub tuam txhab cog lus rau cov neeg siv khoom: los muab kev sib pauv thiab kev pabcuam pub dawb nrog cov neeg siv khoom, thiab muab cov qauv rau cov neeg siv khoom dawb yam tsis muaj nqi coj mus kuaj.
11, Kev Ua tiav tau tsim: Peb lub tuam txhab yav dhau los tau xa 100 tons rau Pakistan.
Koj puas xav nrhiav tus kws tshaj lij ntawm Electrode Paste?
Koj puas xav nrhiav tus neeg muag khoom ruaj khov thiab ntseeg tau?
Tom qab ntawd thov hu rau peb
Hu rau kuv:
Email: wp@cnjingganrefractory.com/sdwenping@163.com
TEL: 86-0533-4188518 / Fax: 86-0533-4188518
Rose: +86-13275332819(wechat/whatsapp tus xov tooj)
Cim npe nrov: electrode paste, Suav teb, manufacturers, lwm tus neeg, Hoobkas, siv, khoom