1, Kev piav qhia ntawm Fly tshauv ntab hlaws
Cov khoom tseem ceeb ntawm ya tshauv ntab hlaws yog silica thiab alumina, nrog rau hluav taws kub ntawm 1600-1700 degree . Lawv yog cov zoo heev kub-kub hluav taws-resistant thiab thermal rwb thaiv tsev cov ntaub ntawv. Fly tshauv ntab hlaws muaj zoo dispersibility, fluidity, siab zog, zoo abrasion tsis kam, hollow spherical zoo, tsis tshua muaj thermal conductivity, zoo thermal rwb thaiv tsev thiab hluav taws xob rwb thaiv tsev, thiab yuav siv tau raws li raw cov ntaub ntawv rau zus tau tej cov khoom insulating nyob rau hauv high kub. Cov khoom siv raw no yog siv dav hauv cov thermal rwb thaiv tsev refractory cib, thermal rwb thaiv tsev txheej, xim txheej, kev tsim kho kev lag luam, nrog rau hauv kev lag luam roj, xws li kev tiv thaiv corrosion thiab thermal rwb thaiv tsev ntawm cov kav dej, thiab palliative ntawm cov roj zoo. drilling av nkos.
2, Kev ua haujlwm tsis zoo ntawm Fly tshauv ntab hlaws

3, Cov yam ntxwv tseem ceeb ntawm cov khoom
1) Tsawg thermal conductivity, 0 054-0.095w/mk, thermal rwb thaiv tsev zoo
2) High hardness, siab zog thiab zoo hnav tsis kam
3) Lub melting point yog ntau tshaj 1400 degree, thiab kub kuj yog zoo
4) PH ≈ 6, zoo acid thiab alkaline tsis kam
5) High dispersion thiab zoo liquidity
4, Lub hom phiaj tseem ceeb ntawm cov khoom
Hluav taws kub resistant, rwb thaiv tsev kub thiab kub rwb thaiv tsev cov ntaub ntawv raw khoom yog siv los tsim hluav taws xob rwb thaiv tsev refractory bricks, tshav kub rwb thaiv tsev coatings, xim additives, lub tsev tshav kub rwb thaiv tsev coatings, roj teb drilling kev lag luam, thiab lwm yam
5, Peb lub tuam txhab cog lus rau cov neeg siv khoom: muab cov kev sib pauv thiab kev pabcuam pub dawb nrog cov neeg siv khoom, thiab muab cov qauv rau cov neeg siv khoom dawb yam tsis muaj nqi coj mus kuaj.
6, Kev Ua tiav tau tsim: Peb lub tuam txhab yav dhau los tau xa 50 tons rau Turkey.
Koj puas xav nrhiav tus kws tshaj lij ntawm Fly tshauv ntab hlaws Khoom?
Koj puas xav nrhiav tus neeg muag khoom ruaj khov thiab ntseeg tau?
Tom qab ntawd thov hu rau peb
Hu rau kuv:
Email: wp@cnjingganrefractory.com/sdwenping@163.com
TEL: 86-0533-4188518 / Fax: 86-0533-4188518
Cim npe nrov: fly-ash ntab hlaws, Tuam Tshoj, manufacturers, lwm tus neeg, Hoobkas, siv, khoom