Cov yam ntxwv ntawm mullite cib

Oct 30, 2021

Mullite bricks muaj siab refractoriness, uas tuaj yeem ncav cuag 1790 ℃. Qhov pib kub ntawm load softening yog 1600 ~ 1700 ℃. Compressive zog ntawm chav tsev kub yog 70 ~ 260MPa. Zoo thermal shock tsis kam. Muaj ob hom sintered mullite cib thiab fused mullite cib. Sintered uas yog ua los ntawm high-alumina bauxite clinker raws li lub ntsiab raw khoom, ntxiv ib tug me me ntawm av nplaum los yog raw bauxite raws li ib tug binder, thiab tsim thiab firing. Fused ituse siab alumina, muaj alumina thiab refractory av nplaum ua raw cov ntaub ntawv, ntxiv charcoal los yog coke nplua particles li txo cov neeg sawv cev, thiab yog tsim los ntawm txo fusion txoj kev tom qab molding.

Lub crystallization ntawm fused mullite loj dua li ntawm sintered mullite, thiab nws cov thermal shock kuj zoo dua li cov khoom sintered. Lawv qhov kub thiab txias ua haujlwm feem ntau yog nyob ntawm cov ntsiab lus ntawm alumina thiab qhov sib xws ntawm mullite theem thiab iav faib. Feem ntau yog siv rau kub moj tej tawg qhov cub sab saum toj, moj tej tawg rauv lub cev thiab hauv qab, regenerator ntawm iav melting rauv, ceramic sintering kiln, tuag kaum rauv hauv ob sab phlu ntawm roj av cracking system, thiab lwm yam.


Xa kev nug