Raws li qhov sib txawv ntawm qhov sib txawv, mullite insulating cib yog mas muab faib ua lub teeb thiab hnyav mullite cib. Raws li kev siv kub sib txawv, lawv feem ntau muab faib ua 1350 mullite insulating cib, 1450 mullite insulating cib, 1550 mullite cib, thiab lwm yam.
Kev ua tau zoo thiab daim ntawv thov ntawm mullite insulating cib: hluav taws kub tsis kam, mus txog 1790 ℃. Thaum pib kub ntawm load softening yog 1600-1700 ℃. Lub cev kub li qub compressive zog yog 70-260 MPa. Zoo thermal poob siab tsis kam. Muaj ob hom sintered mullite cib thiab hluav taws xob melting mullite cib. Lub pob zeb siab mullite yog ua los ntawm bauxite clinker ua cov khoom siv tseem ceeb, cov av me me ntawm cov av nplaum lossis cov bauxite nyoos ua tus binder, thiab tom qab ntawd tsim thiab tua. Mullite cib yog ua los ntawm kev ua kom muaj alumina, muaj alumina thiab av nplaum refractory, ntxiv cov hluav ncaig los sis coke nplua raws li txo tus neeg sawv cev, thiab tom qab ntawv los ntawm kev txo electrofusion. Lub crystallinity ntawm fused mullite yog qhov loj dua qhov ntawm lub siab mullite, thiab nws cov thermal shock tsis kam yog qhov zoo dua li ntawm cov khoom ua txhaum. Lawv lub zog kub ua feem ntau yog nyob ntawm cov ntsiab lus ntawm alumina thiab homogeneity ntawm mullite theem thiab iav faib. Nws yog tsuas yog siv rau hauv cov tshuab ua kom sov lub tshuab ua kom sov sab saum toj, lub cub tawg lub cev thiab hauv qab, iav lub tshuab hluav taws xob rov ua dua tshiab, ceramic sintering rauv, tuag lub tshuab ua kom sov hauv ob sab phlu ntawm cov roj av tawg.