Corundum silicon carbide cib muaj cov thermal conductivity zoo dua, thermal poob siab tsis kam thiab oxidation tsis kam tshaj li ntshiab corundum cib, uas yog, corundum silicon carbide cib tau zoo hnav tsis kam, thermal conductivity, corrosion kuj thiab kub stability. Nws muaj cov txiaj ntsig zoo hauv cov hlau dov cua sov rauv, annealing rauv, incinerator, thee gasification rauv thiab lwm yam.
Cov khoom yog tsim los ntawm electrofusion dawb corundum los yog xim av corundum, electrofusion silicon carbide raws li cov khoom siv tseem ceeb, tsim nyog xaiv cov additives thiab binders, siab - siab molding thiab siab - kub sintering.