Lub tundish sprayed castable yuav tsum ua tau raws li cov kev cai hauv qab no
1.Cov khoom ntawm cov xim pleev xim yuav tsum sib tov sib npaug, tsis muaj sundries raug tso cai sib xyaw, thiab kev thauj mus los hauv cov kav dej yog du.
2.Cov tshuaj tsuag txheej muaj cov dej ntub dej zoo, tuaj yeem tsim cov slurry zoo ib yam nrog dej hauv lub sijhawm luv luv, thiab tau txais cov txheej txheej txau nrog cov tuab tuab nyob rau hauv ib qho kev txau siab.
3.Spray txheej muaj qhov adhesion siab, tsawg rebound, tsis ntws thiab cov plua plav me me
4.Cov tshuaj tsuag txheej hardens sai sai nyob rau hauv qhov kev txiav txim ntawm pov tseg tshav kub ntawm tundish
5.Dry thiab ci tsis tawg thiab tev
6.Cov khoom siv tshuaj tsuag muaj kev tiv thaiv corrosion zoo, thiab cov khoom ntim steel pouring muaj kev nyab xeeb thiab txhim khu kev qha