Cov yam ntxwv ntawm HDPE Geomembrane

Jul 25, 2023

HDPE geomembrane yog impermeable, waterproof thiab puncture resistant. HDPE geomembrane yog ua los ntawm high-density polyethylene cov ntaub ntawv, uas muaj zoo heev ib puag ncig kev nyuaj siab cracking kuj, tsis kub tsis kam, laus kuj, corrosion kuj, ceev ntawm ntau tshaj los yog sib npaug rau 0.94g / cm3, kev pab kub ntawm { {4}} ~ ntxiv rau 60 degree , thiab kev pab cuam lub neej ntawm 50 xyoo. Daim ntawv thov cov khoom lag luam suav nrog cov chaw pov tseg, cov khoom pov tseg pov tseg pov tseg los tiv thaiv cov dej phwj tuaj, cov chaw kho dej phwj tuaj, cov pas dej cuav los tiv thaiv dej, tailings kho anti-seepage, thiab lwm yam.

 

 

 

 

 

 

 

 