Lub teeb ua npuas cib feem ntau yog lub npe hu ua steerating dawb rau kev lag luam pov tseg xws li cov xuab zeb, ya tshauv muaj peev xwm ua pa tsis muaj qhov ntsuas kom sov. Lub teeb ua npuas Cib yog hom kev tiv thaiv ib puag ncig, txuag ib puag ncig, tus nqi qis thermal rwb thaiv tsev cov ntaub ntawv, nrog cov yam ntxwv Suav ib puag ncig. Lub teeb yuag ua npuas cib pob zeb yog ib hom cov khoom lag luam uas muaj zog me me uas muaj cov tshuaj tiv thaiv lub cev me me
Lub teeb ua npuas cov cib muaj cov khoom siv zoo nkauj: lub zog compressive yog ntau dua li {} lub neej, thiab ua npuas dej Cib kuj yog ua los ntawm cov khoom sib txawv. Piv txwv li, ob hom kev ua npuas ncauj kom xis mas ua los ntawm kev sib xyaw ua ke thiab teeb tsa cov nqaij npuas me me nrog cov cement. Lawv muaj qhov zoo ntawm lub teeb hnyav, tso cua sov, rwb thaiv tsev lub suab, kev tiv thaiv hluav taws thiab kev tiv thaiv hluav taws. Tsis tas li ntawd, vim hais tias ntawm kev siv txoj kab uas hla me, tus nqi yog txo qis. Lawv yog qhov zoo tagnrho rau cov neeg tsis thim cov phab ntsa. Autoclaved ua npuas ncauj ua npuas ncauj ntoo cib feem ntau yog ua los ntawm cov cement, hmoov nplej mos thiab dej xuab zeb ua cov khoom nyoos. Tom qab sib tov, nws yog foamed los ntawm nias cua, yuam kom sib tov huab cua rau hauv cov kab sib xyaw ua ke los ua. Cov pob zeb ua nrog Micro Bubble cov qauv raug nrum thiab moulded los ntawm autoclave cov tshuaj tiv thaiv thiab lwm yam txheej txheem. Nws yog cov khoom siv phab ntsa tshiab nrog kev tiv thaiv ib puag ncig, kev txuag hluav taws xob thiab cov khoom muaj zog. Cov tsev siv autoclaved ua npuas ncauj ua thwv cib raws li cov ntaub ntawv phab ntsa tau raug sim ua qhov haujlwm zoo, thiab kev txuag hluav taws xob, tiv thaiv kev tiv thaiv hluav taws thiab lwm yam. Nws tseem yog ua los ntawm cov thwv cib rau cov pob ntsa uas tsis pauv cov phab ntsa.
Cov Khoom Siv Raw: Maas: Txheej Txheem Portland Mortland Mortland Qib 32.5, 42.5, Zoo tib yam Portland Yog tias koj xav ua kom luv luv lub voj voog, koj tuaj yeem siv cov chaw ua kom tawv nqaij nrawm nrawm lossis sulfoaluminate xis mas.
1. Aggrate su: xaiv raws li cov mob hauv zos: Dej xuab zeb, cov hmoov xuab zeb, cov hmoov av), tawg ntub dej slag, tawg rauv tawg, thiab lwm yam.
2. Tus neeg sawv cev ua npuas ncauj: Yx series, cov neeg sawv cev tshwj xeeb rau kev ua npuas.
3. Ntxiv: Siv Yx series, cov tshuaj ntxiv tshwj xeeb rau cov qoob loo ua npuas.
Qhov Zoo:
1. Lub teeb yuag, txo lub tsev thauj khoom: qhuav ntom ntawm 300-1200 kg / msup3 ;, 5-1 / 8.
2. Cov rwb thaiv tsev zoo, rwb thaiv tsev kom sov, thiab lub suab nrov}. {2}}. 16W / mk, thiab lub suab rwb thaiv tsev yog}. 16W / mk, thiab lub suab rwb thaiv tsev
3. Kev ua tau zoo siab ua tau: Lub compressive lub zog yog ntau dua {1}}, thiab lub zog siab tshaj plaws tuaj yeem ncav cuag 10.5 MPA lossis ntau dua.
4. Cov seismic zoo: vim hais tias ua npuas cib yog ib qho khoom siv ntxig, nws muaj qhov ua tau zoo elastic, nws muaj kev nqus tau zoo thiab tshem tawm cov nyhuv zoo ntawm kev poob siab thauj. Nyob rau tib lub sijhawm, ua npuas cib yog sib dua, ua kom muaj kev phom sij rau lub tsev. Tus me dua lub tsev thauj khoom, qhov muaj zog tshaj plaws qhov seismic tiv taus.
5. Tsis muaj kev tawg, lub neej ntev: Ua npuas ncauj cib yuav tsis pom kev tawg thiab hollowing tshwm sim, tsis tas yuav txhuam tus neeg sawv cev, nrog kev ua haujlwm ntev.
6. Cov dej zoo tsis kam: cov dej nqus ntawm cov khoom ua npuas ncauj ua npuas ncauj yog qis dua 22%, uas yog obviously txawv ntawm lwm cov ntaub ntawv phab ntsa.

 

 

 

 

 

 