Ua npuas ncauj ceramic insulation boardis a closed cell ceramic material made mainly from clay tailings, ceramic fragments, river silt, etc., and baked at high temperatures above 1200℃. Nws muaj qhov porosity siab, lub teeb yuag uas tuaj yeem tuav tau los ntawm ob ntiv tes, thiab cov coefficient kub siab dua li cov khoom siv ib txwm muaj. Nws qhov kev ua tau zoo tseem ceeb suav nrog A1 qib hluav taws kub tsis kam, thermal conductivity (0.06 ~ 0.10W / (m · K)), tus nqi nqus dej tsawg, thiab huab cua tsis zoo. Nws tuaj yeem hloov mus rau qhov chaw huab cua los ntawm -50℃txog 200℃thiab muaj kev pabcuam lub neej ntau dua 50 xyoo.
Cov khoom siv no ua tiav cov khoom siv ntsuab los ntawm kev siv cov khoom pov tseg raw khoom (nrog rau kev siv tus nqi ntawm 85%), feem ntau yog siv rau kev tsim cov phab ntsa sab nrauv thiab cov hlua hluav taws xob cais tawm, nrog lub zog sib txuas ntawm ntau dua 5MPa nrog cov cement mortar. Kev tsim kho siv cov cuab yeej nplaum ua ke nrog tus neeg sawv cev cuam tshuam thiab thauj tog rau nkoj kho, thiab qee cov khoom tau raug hloov kho kom muaj dej tsis zoo thiab lub suab- nqus dej ua haujlwm.

Cov khoom tsim nyog rau lub tsev sab nrauv phab ntsa rwb thaiv tsev, hluav taws kev sib cais siv, tsim tus kheej rwb thaiv tsev txias thiab kub choj kev kho mob, thiab lwm yam. Cov khoom muaj hluav taws kub kuj thiab nplaim retardancy, me deformation coefficient, laus kuj, ruaj khov kev kawm, zoo ecological thiab ib puag ncig tiv thaiv, zoo compatibility nrog phab ntsa puag thiab plaster txheej, zoo kev ruaj ntseg thiab stability, thiab yuav siv tau rau tib lub neej raws li lub tsev. Qhov tseem ceeb tshaj, cov khoom muaj qhov ntsuas hluav taws kub ntawm A1, kov yeej qhov tsis muaj zog ntawm cov khoom siv organic ntshai ntawm qhov qhib nplaim taws thiab ua rau muaj kev laus zuj zus, ua rau qhov sib txawv hauv tsev hauv cov khoom siv hluav taws xob tsis zoo rau cov tsev.
Kev Taw Qhia Txog Kev Ua Haujlwm
1. Tsawg thermal conductivity nrog thermal conductivity ntawm 0.06 ~ 0.10W / (MK), piv rau rwb thaiv tsev mortar; Kev ua haujlwm zoo thermal rwb thaiv tsev, tuaj yeem ua cov ntaub ntawv rwb thaiv tsev rau sab nrauv phab ntsa rwb thaiv tsev thiab sab nrauv phab ntsa zoo nkauj panels rau cov tsev nyob sab Europe style.
2. Ua los ntawm siab -kub calcination saum toj 1200 degree, tsis combustible thiab hluav taws kub-resistant, nrog A1 qib combustion kev ua tau zoo thiab hluav taws kub-cov khoom tiv taus zoo ib yam li cov fais fab refractory cib. Nws yog ib qho khoom siv zoo tshaj plaws rau cov kab hluav taws xob sab nraud thiab hluav taws kub - tiv thaiv cov hlua khi nrog kev tiv thaiv hluav taws.
3. Inorganic rwb thaiv tsev cov ntaub ntawv uas ua los ntawm anti- ceramics aging muaj zoo durability, tsis muaj hnub nyoog, thiab muaj tib lifespan li vaj tse, uas yog unparalleled los ntawm cov pa organic rwb thaiv tsev cov ntaub ntawv.
4. Kev sib raug zoo nrog cov cement mortar, pob zeb, thiab lwm yam, txhim khu kev qha kev sib txuas, zoo sib xws coefficient, thiab cov khoom siv hauv tsev ceramic raug rho tawm ntawm qhov kub thiab txias. Nws tsis tawg, deform, los yog shrink nyob rau hauv thermal expansion thiab contraction. Tom qab ob npaug - sab txheej txheej nrog tus neeg sawv cev inorganic, lub zog tensile sib txuas nrog cov cement mortar tuaj yeem ncav cuag tshaj 5MPa.
5. Cov dej nqus dej tsawg, qhov nqus dej tsawg heev, tuaj yeem sib raug zoo nrog cov cement mortar, cov vuas luaj, thiab lwm yam. Cov vuas luaj sab nrauv muaj kev nyab xeeb thiab txhim khu kev qha, tsis txwv los ntawm lub tsev qhov siab, thiab lwm yam.
6. Huab cua tsis kam: Nws tsis deform, muaj hnub nyoog, los yog tawg nyob rau hauv huab cua hnyav xws li raug tshav ntuj, kub thiab txias, thiab cua thiab nag, thiab nws cov kev ua tau zoo yog ruaj khov.
Txoj kev npaj
Cov khoom siv raw rau cov khoom siv hluav taws xob rwb thaiv tsev muaj xws li 30-70 qhov chaw los ntawm qhov hnyav ntawm ya tshauv txhuas seem, 5-15 qhov chaw ntawm talc, 5-15 qhov chaw ntawm kaolin, 30-50 qhov chaw ntawm flux, thiab cov khoom pabcuam suav nrog 0.1-5 qhov chaw ntawm stabilizer, 0.1-5 feem ntawm foaming tus neeg sawv cev 1.-0. Cov khoom siv raw nyiam yog 30-50 feem ntawm ya tshauv txhuas residue, 5-10 qhov chaw ntawm talc, 5-10 qhov chaw ntawm kaolin, thiab 35-50 qhov chaw ntawm flux. SiO2 cov ntsiab lus nyob rau hauv cov txhuas residue rho tawm los ntawm ya tshauv siv yog 30% mus rau 50%, Al2O3 cov ntsiab lus yog 5.0% mus rau 30%, thiab qhov poob ntawm ignition yog 25% mus rau 35%. Cov txheej txheem kev npaj suav nrog kev sib xyaw cov khoom siv raw thiab cov pob ntub dej kom tau cov slurry, ziab cov slurry los ua cov hmoov ua ntej, sintering ntawm 1150℃txog 1200℃rau 30-120 feeb, thiab tom qab ntawd txias. Thaum lub sij hawm sintering txheej txheem, silicon thiab txhuas nyob rau hauv lub txhuas residue muab rho tawm los ntawm ya tshauv teb los ua ib tug mullite theem qauv, uas muab lub foamed ceramic rwb thaiv tsev board siab tensile lub zog.
Glazed foam ceramic insulation board yog tsim los ntawm cov khoom siv raw xws li perlite thiab bentonite, siv ib qho - lub sij hawm sintering txheej txheem thiab siab - kub sintering ntawm 1200 degree, integrating lub functional thiab zoo nkauj txheej ntawm cov khoom.