1, Khoom piav qhia:
1, Direct-bond Magnesite Chrome Brick yog ua los ntawm high purity sintered magnesia thiab chromite nrog SIO2 < 2% thiab sintered ntawm kub (1750 ~ 1800 degree). Cov khoom yog tsim los ntawm periclase thiab magnesia-chromium spinel ua lub ntsiab crystalline theem.
2, Direct-bond Magnesite Chrome Brick muaj ob peb impurities, ncaj qha ua ke ntawm crystalline theem thiab crystalline theem, tsis tshua muaj porosity, siab compressive zog, muaj zog hnav tsis kam, corrosion kuj, thermal shock resistance thiab spalling kuj.
3, Daim ntawv thov ntawm Direct-bond Magnesite Chrome Brick: dav siv nyob rau hauv hluav taws xob arc rauv, tooj liab smelting rauv, refining rauv, cement rotary kiln.Tus nqi ntawm silicate theem nyob rau hauv ncaj qha bonded magnesia chrome cib yog me me, tus nqi ntawm cov thib ob spinel yog loj. , muaj kev sib txuas ncaj qha ntawm periclase thiab periclase, thiab nruab nrab ntawm periclase thiab chromite, yog li ntawd, cov khoom muaj qhov kub thiab txias tsis kam, corrosion kuj thiab thermal shock kuj. ib qho kev daws teeb meem ntawm periclase. Thaum qhov kub thiab txias, MgO-R2O3 thib ob spinel yog tsim, thiab tom qab ntawd tsim cov qauv sib txuas ncaj qha. Direct bonded magnesia chrome cib muaj cov cuab yeej ntawm dai kiln ntawm daim tawv nqaij, yog li nws yog tsim nyog rau nteg firing cheeb tsam ntawm ntau yam cement kilns.
4, Index:
Yam khoom | JD-12 | JD-20 |
MgO% | >60 | >55 |
Cr2O3% yog ' | 12 | 20 |
SIB 2% | <2 | <1.6 |
Cov porosity% | Tsawg dua los yog sib npaug li 18 | Tsawg dua los yog sib npaug li 17 |
PEB g/cm3 | >3.0 | >3.1 |
Txias crushing zog Mpa | >50 | >55 |
Refractoriness nyob rau hauv load degree | >1650 | >1700 |
Thermal expansion tus nqi, 1400 degree, 2hours% | <0.8 | <0.8 |
Thermal shock stability, 950 degree, cua txias, sij hawm | >50 | >50 |

5.Cov lus pom zoo ntawm cov khoom siv tau zoo, cov khoom tau raug xa tawm mus rau Oman, Tebchaws Meskas, Morocco thiab Is Nrias teb.
6.Cov chaw tsim khoom yog cov chaw tsim khoom lag luam thiab tuaj yeem muab cov khoom lag luam ua tiav cov ntaub ntawv ntsuam xyuas lossis cov ntaub ntawv xeem thib peb.
Koj puas xav nrhiav tus kws tshaj lij ntawm cov khoom siv refractory?
Koj puas xav nrhiav tus neeg muag khoom ruaj khov thiab ntseeg tau?
Tom qab ntawd thov hu rau peb
Hu rau kuv:
Email: wp@cnjingganrefractory.com/sdwenping@163.com
TEL: 86-0533-4188518 / Fax: 86-0533-4188518
Rose: +86-13275332819(wechat/whatsapp tus xov tooj)
Cim npe nrov: direct-bond magnesite chrome cib, Tuam Tshoj, manufacturers, lwm tus neeg, Hoobkas, siv, khoom