Hauv kev tsim cov khib nyiab incinerators, txhawm rau txuag lub zog, cov khoom siv thermal thiab cov kav dej yuav tsum tau insulated raws li cov kev cai, thiab cov ntaub ntawv rwb thaiv tsev thiab thickness yuav tsum tau xaiv kom tsim nyog. Cov qauv kev suav suav pom zoo yog:
1) Cov khoom siv cua sov, cov kav dej, cov kav dej thiab lawv cov khoom siv uas muaj ib qho ntawm cov xwm txheej hauv qab no yuav tsum tau rwb thaiv tsev: cov uas muaj qhov kub thiab txias sab nraud siab tshaj 50 degree thiab yuav tsum tau txo cov cua sov; Cov neeg uas xav tau kev tiv thaiv khov, tiv thaiv condensation, los yog ncua nruab nrab condensation; Cov txheej txheem tsis tas yuav tsum tau rwb thaiv tsev, thiab sab nraud qhov kub thiab txias tshaj 60 degree, thaum lwm yam kev ntsuas tsis tuaj yeem coj los tiv thaiv kev kub nyhiab rau cov neeg ua haujlwm;
2) Thaum xam cov rwb thaiv tsev thickness, qhov kub nyob sab hauv tsev feem ntau yog 20 degree, sab nraum zoov ambient kub yog npaum li qhov nruab nrab kub nyob rau hauv lub xyoo, thiab lub anti scald rwb thaiv tsev ambient kub yog npaum li cas raws li qhov nruab nrab kub ntawm lub kub tshaj lub hli. ;
3) Kev xaiv cov ntaub ntawv rwb thaiv tsev:
Cov khoom siv nrog qhov nruab nrab kub siab dua lossis sib npaug li 350 degree yuav tsum tau insulated nrog aluminium silicate fiber, thaum cov khoom siv nrog qhov nruab nrab kub<350 ℃ shall be insulated with rock wool products;
Cov kav dej thiab cov kav dej thiab cov khoom siv nrog lub cheeb ntawm Ntau dua lossis sib npaug ntawm 38mm thiab qhov nruab nrab kub ntawm Ntau dua lossis sib npaug li 350 degree yuav tsum tau insulated nrog aluminium silicate fiber ntau lub plhaub;
Cov kav dej thiab cov kav dej nrog txoj kab uas hla ntawm Ntau dua lossis sib npaug li 38 hli thiab qhov nruab nrab ntawm qhov siab tshaj lossis sib npaug li 50 degree yog insulated nrog pob zeb wool plhaub rwb thaiv tsev;
Cov kav dej thiab cov kav dej thiab cov khoom siv nrog lub cheeb ntawm tsawg dua 38mm yog insulated nrog aluminium silicate fiber ropes; Lub rwb thaiv tsev ntawm lub luj tshib yog ua los ntawm aluminium silicate lossis pob zeb wool cov ntaub ntawv; Cov cua kub duct thiab flue yog insulated nrog pob zeb wool board;
Li qub thiab zoo li tus nrog ib txoj kab uas hla (DN) ntawm ntau dua los yog sib npaug li 40 hli yog nruab nrog tsim rwb thaiv tsev lub tes tsho (xws li txheej sab hauv, lub ntsiab rwb thaiv tsev txheej, thiab txheej tiv thaiv txheej). Cov khoom siv tiv thaiv sab nrauv yog detachable hlau tiv thaiv tawv, kom ntseeg tau tias cov ntaub thaiv npog thiab tuab yog tib yam li cov kav dej uas nws txuas nrog.
Valves nrog DN<40mm are insulated with aluminum silicate fiber rope, with the same insulation thickness as the connected pipeline. The outer protective layer material is 0.1mm thick low alkali glass cloth.