1, Khoom piav qhia:
Siv calcined zoo bauxite ua aggregate thiab ntxiv raw cov ntaub ntawv nrog zoo kub kub kev ua tau zoo li matrix, nyob rau hauv tus txheej txheem ntawm kub sintering thiab kub kev pab cuam, lub matrix qauv ntawm cov khoom tau zoo tuaj, thiab lub siab kub creep tus nqi ntawm cov khoom mus txog. 1550 degree *50h Tsawg dua lossis sib npaug li 0.6%. Nyob rau tib lub sijhawm, cov khoom muaj qhov ntom ntom ntom ntom, cov compaction zoo, tsis tshua muaj qhov hws thiab cov nqi qis ntawm reburning, so Tsawg Creep Rate High Aluminium Cibyog zoo siv nyob rau hauv qhov cub kub.
2, Index:
Al2O3 | A. P | C.C.S | B. D | Nkag hauv qab 0.2Mpa*50h | PLC % | ||
|
|
|
|
| 1550 degree * 2h | ||
Ntau dua lossis sib npaug li 75 | Tsawg dua los yog sib npaug li 20 | Ntau dua lossis sib npaug li 70 | Ntau dua lossis sib npaug rau 2.65 | 1500 degree Tsawg dua lossis sib npaug rau 0.6 | 0.1-0.2 | ||
Ntau dua lossis sib npaug li 70 | Tsawg dua los yog sib npaug li 21 | Ntau tshaj los yog sib npaug rau 60 | Ntau dua lossis sib npaug li 2.55 | 1450 degree Tsawg dua lossis sib npaug li 0.6 | 0.1-0.2 | ||
3, Kev Paub Txog Tsawg Creep Rate High Aluminium Cib:Nyob rau hauv lub hauv paus ntawm high-zoo high-alumina cib cov khoom xyaw, high-temperature kev ua tau zoo raw cov ntaub ntawv yog ntxiv rau lub matrix ntawm cov khoom, thiab kev noj ib theem zuj zus yog nruj me ntsis tswj nyob rau hauv lub mixing txheej txheem los xyuas kom meej superior kev kawm ntawm cov khoom qauv. cov txheej txheem ntawm kub sintering, cov khoom tau tsim ib tug zoo compact qauv, tsis zoo mineral theem ntawm kub thiab ruaj khov zog ntawm qhov kub thiab txias, uas ua rau cov khoom muaj cov yam ntxwv zoo xws li kub tsis kam, creep kuj, tsis tshua muaj linear hloov tus nqi thiab atmospheric corrosion kuj.
4, Daim duab ntawm Tsawg Creep Rate High Aluminium Cib:Lattice Bricks thiab lwm yam
5, Daim Ntawv Thov:Siv nyob rau hauv regenerator ntawm kub moj tej tawg qhov cub, Thaum tshav kub kub exchanger khoom rau lwm yam muaj furnaces
6,Vim tias peb muaj cov cuab yeej tsim khoom zoo tshaj plaws ntawm cov khoom no, peb tuaj yeem tsim cov khoom raws li tus neeg siv cov kev xav tau, cov qauv ntawm cov khoom, tag nrho cov ntsuas ntawm cov khoom raug kuaj ua ntej xa khoom, thiab cov khoom tsis tsim nyog yuav tsis raug tsim.

7, Hais txog peb cov khoom thiab kev siv cov khoom
1) Cov pwm peb siv yog hlau alloy, hnav-tiv taus, thiab cov khoom tsim muaj cov npoo zoo thiab cov fab.
2) Multistage batching yog siv, qhov tseem ceeb particle loj yog tsawg dua los yog sib npaug rau 2.5 hli thiab cov hmoov zoo yog ntau tshaj 180 meshes. Lub matrix ib feem ntawm cov khoom yog cov khoom siv hluavtaws, uas lav qhov siab ceev, siab zog thiab zoo heev kub ua haujlwm ntawm cov khoom.
3) 300-630 tons tsis siv neeg molding tshuab yog siv nyob rau hauv cov khoom molding
4) Qhov kub thiab txias ntawm cov khoom sib txawv ntawm 1450 txog 1480 degree.
5) Cov khoom yog siv nyob rau hauv regenerator ntawm kub moj tej tawg qhov cub, thiab cov nyhuv yog zoo yam tsis muaj qhov txawv txav.
6) Kev xa khoom mus sij hawm ntev rau cov neeg siv khoom siv steel hlau, xa tawm mus rau sab hnub tuaj Asia, Asia, Europe thiab lwm tus neeg siv txawv teb chaws.
7) Kev xa khoom txhua xyoo ntau dua 10, 000 tons
8) Peb muaj cov cuab yeej kuaj xyuas thiab cov khoom zoo, kev tswj xyuas zoo, thiab siv tus qauv ISO90001.
8, Cov khoom ntim:
siv kev nyab xeeb, ruaj khov thiab noo noo-pov thawj packing haum rau kev thauj mus los hauv av thiab hiav txwv
9, Peb qhov kev pabcuam:
1) Muab cov lus qhia pub dawb rau cov neeg siv
2) Pub dawb rau cov neeg siv los muab cov lus piav qhia ntawm cov khoom siv
3) Pub dawb rau cov neeg siv los muab cov khoom tsim qauv tsim qauv
4) Dawb rau cov neeg siv los muab cov qauv, rau cov neeg siv kev sim
10, Peb qhov zoo:
1) Kev tshaj lij, nrog ntau tshaj 20 xyoo ntawm kev tsim khoom thiab kev lag luam, muaj zog sib pauv thiab kev pabcuam
2) Peb muaj peb tus kheej Refractory cov khoom tsim kev koom tes Hoobkas
3) Peb muaj peb tus kheej Graphite Electrode khoom tsim kev koom tes Hoobkas
11.Cov lus pom zoo ntawm cov khoom siv tau zoo, cov khoom tau raug xa tawm mus rau Kaus Lim Qab Teb, Nyiv, Pakistan, Oman, thiab Is Nrias teb.
12.Cov chaw tsim khoom yog cov chaw tsim khoom lag luam thiab tuaj yeem muab cov khoom lag luam ua tiav cov ntaub ntawv ntsuam xyuas lossis cov ntaub ntawv xeem thib peb.
Koj puas xav nrhiav tus kws tshaj lij ntawm cov khoom siv refractory?
Koj puas xav nrhiav tus neeg muag khoom ruaj khov thiab ntseeg tau?
Tom qab ntawd thov hu rau peb
Hu rau kuv: Email: wp@cnjingganrefractory.com/sdwenping@163.com
TEL: 86-0533-4188518 / Fax: 86-0533-4188518
Rose: +86-13275332819(wechat/whatsapp tus xov tooj)
Cim npe nrov: tsawg creep tus nqi siab aluminium cib, Tuam Tshoj, manufacturers, lwm tus neeg, Hoobkas, siv, khoom