Lub tshuab hluav taws xob nruab nrab feem ntau yog siv rau steelmaking thiab ironmaking. Cov ntaub ntawv them nyiaj ntawm lub tshuab hluav taws xob nruab nrab kuj tseem hu ua cov ntaub ntawv hauv ob sab phlu ntawm lub tshuab hluav taws xob nruab nrab, uas tau muab faib ua cov khoom siv acid, nruab nrab thiab alkaline. Cov ntaub ntawv them nyiaj acid yog ua los ntawm high-purity quartz thiab fused silica ua cov ntaub ntawv tseem ceeb, thiab cov khoom siv tsim nyog yog siv los ua tus neeg sawv cev sintering; Cov khoom siv hluav taws xob nruab nrab feem ntau yog ua los ntawm fused corundum, high-purity magnesia, thiab high-purity spinel, nrog cov khoom sib xyaw ua cov sintering agents; Alkaline moj tej tawg rauv cov khoom yog tsuas yog ua los ntawm high-purity magnesium xuab zeb ua lub ntsiab raw khoom, nrog rau tsim nyog additives li sintering agents.
Thaum siv lub tshuab hluav taws xob nruab nrab, nws yog ib qho tsim nyog los pib lub qhov cub. Kev tshuaj xyuas cov khoom thiab kev npaj rau qhov nruab nrab zaus rauv:
1. Cov khoom siv rau cua sov: crucibles, refractory asbestos daim ntaub, cov ntaub ntawv qhuav hauv ob sab phlu, iav dej, breathable cib, thiab lwm yam;
2. Npaj crucibles thiab lwm yam ntaub ntawv raws li qhov ntev thiab ntau npaum li cas nyob rau hauv Daim Ntawv Ntxiv 1 thiab 2 rau ntau hom cub tawg;
3. Lub ellipticity ntawm lub crucible yuav tsum tau raws li qhov yuav tsum tau ntawm Daim Ntawv Ntxiv 1, thiab yuav tsum tsis txhob muaj qhov loj me ntawm qhov chaw sab nrauv. Nws yuav tsum muaj ntau qhov chaw ua pa. Lub crucible yuav tsum tau siv tom qab ntxuav cov xeb ntawm sab nrauv;
4. Lub ntim ntawm cov khoom qhuav yuav tsum tsis txhob puas los yog ntub dej ua ntej siv;
5. Tshawb xyuas qhov muaj cov hlau me me thiab lwm yam khoom sib nqus, nrog rau cov khoom tsis huv hauv cov khoom qhuav; Yog tias muaj, phau ntawv qhia yuav tsum qhia qhov xwm txheej raws sijhawm thiab siv nws lossis tsis ua tom qab ua tiav. Nws yog nruj me ntsis txwv tsis pub nqa cov khoom sib nqus thiab ntau qhov kev suav nrog rau hauv cov khoom siv hauv lub tshuab hluav taws xob;
6. Ua ntej txhim kho lub cib breathable, xyuas seb nws puas ua pa thiab seb puas muaj kev nyab xeeb uas yuav cuam tshuam rau nws txoj kev siv, xws li kev puas tsuaj. Lub cib ua pa yuav tsum tsis muaj qhov tsis zoo thiab tsis muaj qhov tsis zoo, thiab cov yeeb nkab breathable yuav tsum tau ua los ntawm stainless hlau.