1, Taw qhia ntawm Anti-skid Ceramic Roller Bar Rau Cov Menyuam Kiln
Cov khoom yog tsim los ntawm cov av nkos drilling thiab yeeb nkab extrusion, cov tsos zoo thiab lub zog ntawm cov khoom yog superior rau ntawm grouting.Qhov saum npoo ntawm cov khoom yog ua tiav rau hauv cov kab txaij, uas zoo txhim kho cov kev ua haujlwm tsis zoo, txo kev sib tsoo thiab tsis Hloov kev tsav tsheb thaum lub sij hawm siv cov khoom, thiab txhim kho kev siv cov nyhuv.Txhua qhov kawg ntawm cov khoom muaj ib los yog ob lub qhov qhib, uas pab txhawb thiab txhim kho kev sib kis tau zoo.Qhov sib ntxiv ntawm 7-15% zirconium oxide hauv cov khoom txhim kho qhov kub thiab txias tsis kam thiab hnav tsis kam ntawm cov khoom, thiab txhim kho lub sijhawm siv tau zoo.
2, Cov yam ntxwv ntawm Anti-skid Ceramic Roller Bar Rau Cov Menyuam Kiln
1) Cov khoom yog zirconium ceramic rollers, anti-skid, kub resistant, thiab cov kev pab cuam kub yog 1450 degree.
2) Zoo thermal shock stability, tsis muaj cracking.
3) High flexural zog, puag ncig, ncaj thiab tsis yooj yim rau khoov.
4) Tsis tshua muaj dej nqus, hluav taws kub tsis kam, kub tsis kam thiab hnav tsis kam.
3, Daim ntawv thov Anti-skid Ceramic Roller Bar Rau Cov Menyuam Kiln
Siv nyob rau hauv kub kub ceramic pobzeb cov menyuam kiln, kub kub ceramic rau cov kiln, siab load khoom rau cov menyuam kiln, thiab lwm yam.
4, Index:
Yam khoom | JZHB-15 |
Al2O3% | >70 |
ZrO2% | 7-15 |
Fe 2O3% | <0.3 |
Qhov ntom ntom g / cm3 | >2.7 |
Pom tseeb porosity% | Tsawg dua los yog sib npaug rau 19 |
Kev nqus dej% | Tsawg dua los yog sib npaug li 8 |
Khoov zog Mpa | 25 qib 70 |
1350 degree 60 | |
Ua haujlwm kub degree | 1430 |
5, Khoom duab
6.Zoo tawm tswv yim ntawm cov khoom siv nyhuv, cov khoom tau raug xa tawm mus rau South Kauslim, Pakistan, Russia
7. Covcov chaw tsim khoom yog cov chaw tsim khoom lag luam thiab tuaj yeem muab cov khoom lag luam ua tiav cov ntaub ntawv ntsuam xyuas lossis cov ntaub ntawv xeem thib peb.
Koj puas xav nrhiav ib tus kws tshaj lij ntawm Anti-skid Ceramic Roller khoom?
Koj puas xav nrhiav tus neeg muag khoom ruaj khov thiab ntseeg tau?
Tom qab ntawd thov hu rau peb
Hu rau kuv:
Email: wp@cnjingganrefractory.com/sdwenping@163.com
TEL: 86-0533-4188518 / Fax: 86-0533-4188518
Rose: +86-13275332819(wechat/whatsapp tus xov tooj)
Cim npe nrov: anti-skid ceramic roller bar rau cov menyuam kiln, Tuam Tshoj, manufacturers, lwm tus neeg, Hoobkas, siv, khoom