Tsev > Xov xwm > Ntsiab lus

Kev txuam nrog thiab kev siv cov ntaub ntawv refractory rau ua ntej decomposition kiln

Nov 20, 2025

Kev txuam nrog thiab kev siv cov ntaub ntawv refractory rau ua ntej decomposition kiln
Thaum lub sijhawm ua haujlwm thiab siv cov pob zeb qeeb, Recractory Cib tsuas yog siv ob hom kev ntxhov siab ntawm cov kiln thiab axial compression kev ntxhov siab raws cov lus KILN.
Lub radial shear kev ntxhov siab tsuas yog los ntawm kev tawm dag zog tshuab tsim tsim tau thaum lub sijhawm ua haujlwm ntawm lub teb chaws cub. Lub Kiln Barrel yuav yauv tsis txaus ntseeg, thiab nruab nrab ntawm lub thoob yuav tsis muaj ib txoj kab ncaj; Ntawm qhov tod tes, hauv thaj chaw ze ntawm lub log txhawb log, lub cev ntawm lub cev me yuav dhau los ntawm elliptical deformation. Kev ntsuas xyuas cov khoom siv khiav ntawm cov qauv Kiln uas siv qhov sib txawv ntawm lub cev tuaj yeem ncav cuag 0.6 ‰ rau 0.7 ‰ ntawm cov khoom loj. Raws li txoj kab uas hla ntawm Elliptical Kiln nce thiab Kiln Ceev Accelerates, lub sij hawm ua hauj lwm nrawm rau ntawm lub cev ua kom muaj zog. Cov refractory bricks yuav raug rau kev puas tsuaj radial haub kev puas tsuaj, thiab thaj chaw hloov chaw sab nraud yog thaj chaw ntawm radial shear kev ntxhov siab * *.
Muaj ob qho tseem ceeb rau lub cim ntawm axial compressive kev ntxhov siab. Ib qho laj thawj yog tias cov ntaub ntawv sab hauv lub Kiln txav los ntawm Kiln Tail mus rau lub zog txav ntawm lub zog txav ntawm lub zog txav mus los ntawm lub zog txav mus los hauv qab ntawm lub zog txav ntawm lub pob zeb uas muaj axial; Qhov thib ob yog lub zog nthuav dav tsim los ntawm cov cua sov ntawm cov cib ntau. Kev nthuav dav coefficient ntawm refractory cib ntawm 1400-1450 Qib yog 1.4 ‰ -1.6 ‰. Feem ntau siv ntev ntawm txhua lub cib yog 198mm, thiab ntsuas kev nthuav dav yog 2.8-3.2mm. Yog tias tus nqi cua sov dhau nrawm nrawm nrawm nrawm nrawm, tus nqi nthuav dav ntawm cov cib, uas yuav txwv tsis pub muaj kev ntxhov siab ntxiv, txawm tias ua rau cib tawg. Qhov kev ua haujlwm hnyav ua haujlwm sab hauv lub Kilno yuav tsum muaj cov cib rectractory kom muaj kev siv zog muaj zog. Nyob rau tib lub sijhawm, tsim nyog cia cov pob qij txha nthuav tawm thaum kiln cib alasonry tuaj yeem ua tau zoo rau kev puas tsuaj los ntawm ob qhov kev ntxhov siab no.
Thermal Kev Nyuaj Siab Kev Puas: Cov txiaj ntsig kev ntsuas kub qhia tau tias qhov chaw kub ntawm ib qho kev sib hloov, thiab qhov tshwm sim thermal no yog ib qho ntawm kev puas tsuaj ntawm kev regractory cib. Nrog tus qauv ntawm loj {2} txoj kab kev lag luam sab nraud, lub cheeb tsam sab nraud tau nce ntxiv (ntawm cov kab ntau ntxiv mus rau lub zog thib peb nrog kev nce ntawm lub taub dej. Lub Volumetric cov zis tau nce ntxiv rau ntau tshaj peb zaug ntawm cov khoom siv ib txwm muaj, ncav 5t / m3. D). Qhov no tsis tsuas yog nce cov neeg kho tshuab kev ntxhov siab, tab sis kuj tseem ua rau lub zog thermal sab hauv lub kiln. Chav tsev kub thauj ntawm cov cib regractory kuj nce, thiab kev siv hluav taws xob ua kom muaj zog. Ib qho ntxiv, Kiln nrawm kuj tau nce (3-4 r / min), uas yuav tsum tau ntau dua ntawm cov pa hluav taws kub uas tau muaj kev regractory kom muaj zoo dua thermal poob taus.
Tshuaj yaig kev puas tsuaj: tshuaj yaig yog ib qho ua rau muaj kev puas tsuaj rau kev puas tsuaj. Ntawm qhov kub ntawm 1350-1450℃sab hauv lub kiln, clinker nrog muaj zog alkalinity yuav ua rau muaj zog tshuaj cenposion rau lub Kiln. Cov theem ua kua hauv lub clinker yuav hnov ​​qab zib cov ntsev raws li cov ntsev ua kua qaub rau hauv lub qhov tob ntawm 40-50mm. Qhov no yuav ua rau cov qauv ntawm lub cib ua kom tawg, nyuaj, xoob, thiab nquag nquag tev. Tus yuam sij kom dhau kev puas tsuaj los ntawm kev puas tsuaj los ntawm kev siv tshuaj yaig yog los tiv thaiv kev nkag mus rau qee yam hauv xissents hauv Maas (Sio2, Cao, KCI, thiab lwm yam). Ib qho ntxiv, cov khoom siv tsis zoo xws li alkali, chlorine, thiab leej faj hauv cov ntaub ntawv raw kuj tseem ua rau muaj kev phom sij thiab kev puas tsuaj rau lub kilning. Cov sulfates thiab tshuaj lom neeg ntawm alkali yog unriched tsis tu ncua los ntawm kev hloov pauv, hws, thiab rov qab ncig ua ntej. Feem ntau, piv nrog cov thawj cov khoom siv ua ntej, cov chlori, chlorine, thiab sulfur txhawb dej nyob rau hauv cov kub ntawm 5 zaug, 80-100 zaug, thiab 3-5 zaug feem. Cov khoom siv refractory yog eroded los ntawm alkali teb los ntawm cov khoom siv hauv caug thiab ua kom muaj cov zaub mov nthuav dav thiab teeling, ua rau alkali tawg thiab ua kom puas.
Tsim nyog siv cov khoom siv refractory: thaum xaj cov ntaub ntawv refractory, nws yog ib qho tseem ceeb kom paub meej tias lawv ntev - tsis muaj kev nyab xeeb. Firstly, xav txog cov kev tsim nyog thiab kev siv cov peev txheej ntawm cov chaw tsim khoom, thiab them sai sai {{2} Kev muag khoom ntawm cov ntaub ntawv refractory. Thaum kev txiav txim siab refractory, yuav tsum tau ua rau kev ntim khoom thiab tsheb thauj khoom ntawm cov khoom siv khoom noj. Yog tias tsis muaj lub ntim khoom khov thiab ruaj khov, kev thauj mus los zoo tuaj yeem yooj yim ua rau puas tsuaj thiab cuam tshuam rau lub neej pabcuam. Rau cov ntaub ntawv refractory nrog txee lub neej (xws li qee cov khoom siv cas), ntev}} lub sij hawm cia yuav tsum zam. Refract txoj kev cib yuav tsum yog ya raws- pov thawj thiab muab cov ntawv pov thawj rau kev ua kom tsis meej pem. Txhim kho qhov zoo ntawm Masonry kev tsim kho: Qhov zoo ntawm cov khoom siv ua haujlwm ntawm Masonry kev tsim kho yog qhov txuas tseem ceeb hauv kev ua kom zoo ntawm kiling. Cov "kev cai ntawm kev siv cov ntaub ntawv refractory rau CAs lub pob zeb qeeb qeeb" tshaj tawm thiab siv nyob rau xyoo 1995 muab kev tsim kho qauv. Cov kev lag luam yuav tsum muaj kev cob qhia rau kev siv hluav taws xob ua haujlwm, txhawm rau txhim kho cov neeg ua haujlwm tsim kho. Txawm li cas los xij, vim muaj ntau yam, muaj ntau feem ntau qhov tshwm sim ntawm tsis {14} Taug kev thaum lub sijhawm kev tsim kho, uas yuav tsum ua haujlwm hauv kev tswj hwm. Cov txheej txheem kev tsim kho Masonry yuav tsum tau them nyiaj rau cov teeb meem hauv qab no: tswj cov dej ntxiv raws li yuav tsum tau ua. Txawm hais tias muaj cov dej loj yog qhov yooj yim rau kev tsim kho, nws zoo heev txo lub zog ua tau zoo ntawm cov khoom siv casting. Them sai sai rau kev tsim kho vaj tse. Cov xwm txheej tshwm sim yog qhov kev tsim kho, txhawm rau ntes cov sijhawm, kom muaj kev tsim khoom noj thaum ntxov, tsis tshua muaj tswj kom muaj cov ntaub ntawv casting raws li lub sijhawm. Qhov no yuav inevitably ncaj qha cuam tshuam nws txoj kev ua tau zoo. Thaum cua sov thiab ci cov khoom siv tom qab kev tsim kho, kev teeb tsa ntawm kev sab nraud lub qhov yuav tsum tau txiav txim siab, tshwj xeeb tshaj yog nyob rau thaj chaw Hood cheeb tsam. Feem ntau, tsis muaj nyias cov txheej txheem sib cais ntawm qhov chaw no, thiab qhov kub ntawm cov kub clinker nkag los ntawm ib puag ncig 400℃rau ib puag ncig 1100 degree. Yog tias lub qhov tso tawm tsis yog teeb tsa kom raug, kev pheej hmoo ntawm cov khoom siv refractory tawg tau siab heev. Lub sijhawm Masonry, cov Cib Meem yuav tsum tsis muaj cov ntsiab lus tshem tawm lossis chaw. Lub taub hau loj yuav tsum tau nias kom nruj rau lub tog raj kheej, thiab cov leeg weld weld yuav tsum muaj polished tiaj. Qhov deformed ib feem ntawm lub tog raj kheej yuav tsum tau ua kom zoo thiab ua kom haum nrog cov av nplaum pads. Tawm cov pob qij txha nthuav dav raws li kev nthuav dav coefficient ntawm cov cib. Tawm hauv ntau qhov khoob tuaj yeem ua rau cib teeb thiab txawm tias brick zuaj plaub hau, thaum tawm ntawm cov tsis txaus ntseeg tuaj yeem ua rau muaj kev ntxhov siab. Kev siv ntawm kev kho cov phiaj hlau yuav tsum tau ua qauv. Qhov ntau npaum li cas yuav tsum tsis txhob muaj ntau dhau, thiab nws yog qhov tsis muaj cov npoj yaig loj thiab nws tsis pub nws xaws thiab nws tsis pub xaws; Daim phiaj hlau yuav tsum tsis txhob tso ib nrab rau hauv cov pob txha sib koom ua ke, ua rau qhov me me sib koom ua ke kom nruj thiab ua ke loj kawg kom xoob; Thaum ntxig cov hlau phaj, tsis txhob quab yuam smash nws, thiab tsis txhob ntaus lossis khoov cov hlau phaj kom puas tsuaj rau lub cib npoo. Siv cov roj hmab rauj lossis ntoo ntoo kom tua lub cib nplaim, kom ntseeg tau tias cov cib no tau sib chwv. Kev siv tsim nyog thiab kev ua haujlwm, Kiln cua sov. ** Firstly, raws li kev ua yeeb yam ntawm Refractory cib, feem ntau txoj kev xav ua kom nruj (h) kom nruj kev puas tsuaj rau kev puas tsuaj los ntawm kev ntxhov siab ntawm thermal; Nyob rau tib lub sijhawm, nruj me ntsis ua cov kiln cua sov thiab txoj siav kom txo cov tshuab kev puas tsuaj los ntawm kev siv tshuab ntawm cov cib. Thaum lub hauv paus kub me tshiab yog ci, nws yog qhov nyuaj rau kev tswj hwm kev hloov pauv, uas tuaj yeem ua rau cov roj kub kom poob ntsej muag, uas ua kom muaj kev ntxhov siab rau kev ntxhov siab.

Xa kev nug