Cov Khoom Siv Zoo Rau Masonry Ntawm Refractory Cov Khoom Siv Rau Coke Cub Lub Cev
Qhov Ua Tau Zoo Rau Coke Cub Masonry
① Cib Sib Tham
Qhov cub Coke Masonry yog ua los ntawm ib leeg refractory cib. Refractory slurry feem ntau tsis yooj yim rau sinter zoo nyob rau hauv qis dua ntawm qhov cub hluav taws xob ntawm cov cua sov lub cev ntawm qis dua kub. Txawm hais tias nws yog sintered nyob rau sab qaum kev ntawm lub rauv taws, nws lub zog tsis yog siab, yog li cov pob qij txha ua kom tsis muaj zog hauv Masonry. Txhawm rau kom nce qhov nruj ntawm Coke cub Masonry, txawm hais tias ntau cov cib xwm txheej tsis xwm yeem siv, cov pob qij txha tseem yuav tsum muaj tag nrho thiab nruj. Cov pob qij txha yuav tsum tsis txhob ua kom dav heev, txwv tsis pub nws yuav tsis muaj zog, tsis yog ib qho yooj yim rau kev sib tw thiab txo lub zog ntawm masonry. Raws li kev xyaum, cug lub tshuaj sib koom ua ke ntawm 3-6mm yog qhov haum ntau ntxiv, uas tuaj yeem ua tiav cov tshuaj pleev ib ce puv pob qij txha thaum lub sijhawm Masonry thiab ua tau raws li cov kev xav tau ntawm cov tshuab ua khoom.
Txhawm rau kom ua tiav cov pob qij txha tag nrho, cov coke cub bricklaying tsim nyog, muab cov hlua khi ua ke, tab tom muab cov hlua khi ua ke, thiab nias cov cib pob qij txha los ntawm kev sib tw.
② Kev nthuav dav thiab zawv zawg txheej
Masonry undergoes tseem ceeb nthuav los ntawm lub chaw txias rau lub xeev kub. Qhov ntev ntawm cov pa roj caramber nthuav dav ntawm qhov chaw sab nraud, thiab qhov kev nthuav dav ntev ntawm kev nthuav dav lub cev tseem tsis hloov pauv hauv kev tsim khoom. Yog li ntawd, qhov dav ntawm kev nthuav dav sib koom tes yuav tsum tau yoog raws li tus nqi nthuav dav los ntawm cov cua kub ntawm masonry. Cov khoom siv kub thiab cov khoom siv refractory uas siv rau cov cheeb tsam sib txawv sib txawv, ua rau muaj kev nthuav dav sib txawv thiab tus lej thiab cov pob qij txha sib npaug sab hauv txhua thaj chaw. Qhov kev nthuav dav ntawm thaj tsam ntawm Silica Cork Cork tuaj yeem suav tau ntawm 2%, lossis 20 hli rau ntawm kev sib koom ua ke ntawm cov hmoov tshauv). Ib qho kev nthuav dav me me tuaj yeem ua rau muaj kev sib koom ua ke, deformation, lossis tawg ntawm Masonry; Yog tias nws loj dhau lawm, tseem yuav yog qhov khoob tom qab kev nthuav dav, uas tuaj yeem ua rau yooj yim. Qhov zoo tshaj ntawm cov pob qij txha nthuav dav yog tsuas yog ua kom tau los ntawm qhov dav ntawm kev sib koom tes thiab lub tiaj tiaj ntawm phab ntsa sib zog. Yog li ntawd, nws yog qhov yuav tsum tau siv cov kev nthuav dav sib koom ua ke rau Masonry, nrog ib thickness 1-2mm me dua qhov dav ntawm kev nthuav dav. Txhawm rau kom muaj lub ntsej muag ntawm cov phab ntsa sib koom ua ke, lub cib nplaim uas nyob ib sab ntawm kev nthuav dav yuav tsum yog tiaj tus ua ke, feem ntau yog siv tshuab ua. Cov pob qij txha nthuav dav yuav tsum muaj cov khoom siv raws li qhov dav ntawm kev sib koom ua ke. Thaum cov kis tau nqaim, siv cov ntawv nees thaum pw cov thwv cib; Thaum qhov kis tau dav, siv ib qho kev nthuav dav sib koom ua ke los tsim nws, ntxuav nws, sau nws nrog sawdust, thiab muab hliv asphalt. Sawdust yuav tsum qhuav, huv, thiab dawb ntawm lwm cov impurities. Qhov muag muag taw tes ntawm asphalt yuav tsum tsim nyog, feem ntau ntawm 65-80 degree.
Kev siv ntawm kev nthuav dav sib luag los nqus cov kev nthuav dav ntawm cov cub hluav taws xob ua tiav los ntawm kev sib txheeb ntawm lub masonry ntawm ob sab. Yog li ntawd, ib qho txheej zawv zawg yuav tsum muab tso rau saum cov ntawv nthuav tawm, feem ntau yog siv cov ntawv sau cia hauv cov ntawv nthuav tawm kom tso cai rau kev txav mus los. Qhov ntev ntawm daim ntawv siv rau kev tso cov txheej swb yuav tsum tau npog cov khoom sib xyaw ntawm cov txheej txheem sib xyaw ua ke thaum tso cov txheej txheem ntawm cov txheej txheem sab saud, uas yuav cuam tshuam rau lub zawv zawg ntawm cov masonry; Lwm qhov kawg ncua rau ntawm ntug kev nthuav dav sab saud los tiv thaiv cov ntawv los ntawm kev sib koom ua ke sab saud, uas yuav cuam tshuam qhov zoo ntawm cov txheej swb.
③ Florness, ntsug, thiab nce siab yuam kev ntawm Masonry
Vim tias lub installation ntawm ntau coke cub khoom tom qab ua tiav ntawm cov hluav taws xob lub cev me me ntawm cov txheej txheem sib xyaw ua ke hauv kev ua haujlwm nrog cov cuab yeej siv hluav taws xob ntau lawm.
Qhov kev ua yuam kev ntawm Masonry yog hais txog qhov sib txawv ntawm cov cib txheej nce thiab nce ntawm txheej ntawm cib. Qhov ua yuam kev nyob rau hauv kev nce siab tuaj yeem siv los ntsuas seb tus Masonry raug raws li cov qauv tsim nyog tau ua thiab kev sib koom tes nrog cov khoom siv coke. Qhov nce ntawm Masonry yuav tsum tau ntsuas tsis tu ncua nrog kev tshuaj ntsuam xyuas uas siv tau los ntawm kev sib piv nrog tus kav tus ntsuj plig lossis tus pas nrig.
Lub tiaj tus ntawm Masonry hais txog qib ntawm kev tsis sib xws nyob rau saum npoo ntawm ib qho chaw ntawm ib qho ntawm masonry siv 2m ntev tus pas neeg tus pas ntsuas.
Qhov tseeb ntawm Masonry hais txog qib uas cov dav hlau ntsug ntawm lub masonry deviates los ntawm txoj kab ntsug. Feem ntau ntsuas siv tus txheej txheem plumb BOB.
Txawm hais tias kev hloov pauv ntawm qee qhov xwm txheej, uas yog, lub tiaj ntawm cov ntsug ntawm Masonry yog suav nrog kev sib tw ntawm cov nplaim hluav taws xob ntawm no saum npoo. Thaum lub tiaj tiaj tiaj tsis zoo, cov kev ntsug yog kuj tsis zoo, tab sis qhov yuam kev nyob rau hauv kev ntsug thiab flatness yuav tsis zoo ib yam.
Qhov ntsuas ntawm phab ntsa yog ib qho ntawm cov ntsuas tseem ceeb rau kev ntsuas qhov zoo ntawm Masonry, tshwj xeeb tshaj yog rau cov pa roj caramber. Kev nyuaj siab heev nyob rau hauv kev sib cav sib ceg thiab flatness yuav ua rau bushing coke thiab ua rau kev puas tsuaj ntxov rau lub rauv phab ntsa.
④ Qhov loj me ntawm txhua tus pore thiab nruab nrab ntawm txhua tus pore hauv Coke Cub
Tus ntoo khaub lig- ntu ntu thiab kev sib nrig sib qhov ntev ntawm txhua feem ntawm COKE Cub Masonry kuj yog ib qho ntawm cov ntsuas tseem ceeb rau kev ntsuas qhov zoo ntawm kev ua pob txha. Qee tus yuav cuam tshuam cov kev teeb tsa du ntawm cov cuab yeej tom qab muab kev tsim kho, thaum lwm tus tseem ceeb heev rau kev tswj qhov kub thiab txias rau kev tswj qhov kub thiab txias thaum lub sij hawm ntau lawm. Yog li ntawd, ntxiv rau kev them nyiaj rau kev ntaus pob txha, kev soj ntsuam nruj thiab xaiv Recractory Cib qhov ntev yuav tsum tau ua.