Kev Tsim Khoom Thiab Kev Siv Magnesia Chrome Cib

May 16, 2022

Cov ntaub ntawv tseem ceeb rau kev tsim cov magnesia chrome cib yog magnesia, chrome ore, hluavtaws magnesia chrome xuab zeb thiab additives. Thaum qhov piv ntawm chrome ore rau magnesia yog 50: 50, cov khoom muaj qhov siab tshaj plaws thermal shock stability. Qhov nce ntawm chrome ore cov ntsiab lus yuav ua rau kom nrawm nrawm ntawm ntim. Ua kom muaj cov ntsiab lus magnesia hauv cov khoom siv tuaj yeem txhim kho cov slag tsis kam ntawm cov khoom. Magnesia chrome cib yuav tsum raug rho tawm haujlwm hauv qhov chaw tsis muaj zog oxidizing ntawm 1550-1600 degree .

Magnesia chrome cib yog alkaline qib high-qib refractory nrog hluav taws kub siab tshaj 2000 degree, hluav taws kub tsis kam siab tshaj 2000 degree, thiab cov khoom muag muag feem ntau ntau dua 1550 degree. Nws muaj qhov kub-kub ntim ruaj khov thiab zoo thermal shock stability dua li magnesia cib. Nws yog dav siv hauv metallurgy, tshuaj lom neeg kev lag luam, iav, cement thiab lwm yam lag luam.