Sintered corundum cib txhais tau hais tias cov ntsiab lus ntawm Al2O3 yog ntau tshaj 90 feem pua, thiab lub ntsiab crystalline theem yog - Al2O3 refractory cib. Sintered corundum cib muaj kub tsis kam, siab hardness, oxidation tsis kam, corrosion kuj thiab zoo huab cua nruj. Yog li ntawd, nws muaj ntau yam kev siv.
Hauv kev tsim cov sintered corundum cib, mullite clinker yuav tsum tau ntxiv txhawm rau txhawm rau txhim kho nws cov thermal shock stability thiab slag kuj.
Txhawm rau txo qhov kub thiab txias, 1-2 feem pua TiO2 txhawb nqa feem ntau ntxiv. Cov khoom tuaj yeem raug rho tawm haujlwm ntawm 1550-1600 degree . MgO tuaj yeem cuam tshuam cov qoob loo loj hlob thiab tau txais cov qauv microcrystalline, uas yog qhov zoo los txhim kho lub zog ntawm cov khoom siv.
Technical Performance index ntawm sintered corundum cib