Tsev > Xov xwm > Ntsiab lus

Ntau Lawm Thiab Cov Khoom Ntawm Sintered Corundum Cib

May 30, 2022

Sintered corundum cib txhais tau hais tias cov ntsiab lus ntawm Al2O3 yog ntau tshaj 90 feem pua, thiab lub ntsiab crystalline theem yog - Al2O3 refractory cib. Sintered corundum cib yog dav siv vim nws qhov kub tsis kam, siab hardness, siab zog, oxidation kuj, corrosion kuj thiab zoo huab cua nruj.

Hauv kev tsim cov sintered corundum cib, mullite clinker yuav tsum tau ntxiv los txhim kho nws cov thermal shock stability thiab slag kuj.

Txhawm rau txo qhov kub thiab txias, 1-2 feem pua ​​​​ntawm TiO2 txhawb nqa feem ntau ntxiv. Cov khoom tuaj yeem raug rho tawm haujlwm ntawm 1550-1600 degree . MgO ntxiv rau inhibit qhov kev loj hlob ntawm cov nplej thiab tau txais cov qauv microcrystalline, uas muaj txiaj ntsig zoo los txhim kho lub zog ntawm cov khoom.