Txheej txheem tsim khoom ntawm MgO-C cib

Jul 29, 2026

Cov txheej txheem tsim khoom ntawm MgO-C bricks

 

Cov ntaub ntawv tseem ceeb rau MgO-C cib suav nrog fused magnesia lossis sintered magnesia, flake graphite, organic binders, thiab antioxidants.

Magnesia
Magnesia yog cov khoom siv tseem ceeb rau kev tsim MgO-C cib, muaj nyob rau hauv fused magnesia thiab sintered magnesia cov ntaub ntawv. Piv nrog rau sintered magnesia, fused magnesia muaj qhov zoo xws li cov pob zeb periclase loj dua thiab ntau dua qhov ntom ntom, ua rau nws nyiam cov khoom siv raw rau MgO-C cib ntau lawm. Rau kev tsim cov magnesia zoo tib yam-raws li refractories, lub ntsiab yuav tsum tau rau magnesia raw cov ntaub ntawv yog siab- kub lub zog thiab corrosion kuj, yog li hais txog purity ntawm magnesia thiab C/S piv thiab B₂O₃ cov ntsiab lus nyob rau hauv nws cov tshuaj muaj pes tsawg leeg. Nrog rau txoj kev loj hlob ntawm kev lag luam metallurgical thiab nce hnyav smelting tej yam kev mob, cov magnesia siv nyob rau hauv MgO-C cib rau metallurgical khoom (converters, hluav taws xob furnaces, ladles, thiab lwm yam) yuav tsum tsis tau tsuas yog cov tshuaj muaj pes tsawg leeg, tab sis kuj siab ceev thiab loj crystallite loj nyob rau hauv cov nqe lus ntawm microstructure.

 

Kev tsim cov txheej txheem ntawm magnesia carbon brickCarbon Source
Txawm hais tias nyob rau hauv ib txwm MgO-C cib los yog dav siv qis-carbon MgO-C cib, flake graphite feem ntau yog siv los ua cov pa roj carbon. Graphite yog ib qho tseem ceeb raw khoom rau MgO-C cib, feem ntau yog vim nws lub cev zoo heev: ① non-wettability los ntawm slag; ② siab thermal conductivity; ③ Tsawg thermal expansion. Tsis tas li ntawd, graphite tsis dhau eutectic melting nrog refractories ntawm qhov kub thiab txias thiab muaj siab refractoriness. Qhov purity ntawm graphite cuam tshuam rau kev ua haujlwm ntawm MgO-C bricks; Feem ntau, graphite nrog cov ntsiab lus carbon ntau dua 95%, nyiam dua ntau dua 98%, yog xav tau.

Ntxiv nrog rau graphite, cov pa roj carbon dub kuj yog feem ntau siv hauv kev tsim cov magnesia-carbon cib. Cov pa roj carbon dub yog cov khoom tawg yooj yim heev ntawm cov hmoov carbonaceous uas ua los ntawm thermal decomposition lossis tsis tiav combustion ntawm hydrocarbon tebchaw. Nws muaj cov khoom zoo (tsawg dua 1 μm), thaj chaw loj tshwj xeeb, cov ntsiab lus carbon ntawm 90-99%, siab purity, siab hluav taws xob tiv thaiv, siab thermal stability, thiab thermal conductivity kuj tsis tshua muaj, koom nrog cov khoom tsis yog -graphitizing carbon. Qhov sib ntxiv ntawm cov pa roj carbon dub tuaj yeem txhim kho qhov kev tiv thaiv tsis zoo ntawm MgO-C cib, ua kom cov pa roj carbon ntau ntxiv, thiab txhim kho cib ntom ntom.

Binder
Cov binders feem ntau siv hauv MgO-C cib tsim muaj xws li thee tar, thee tar pitch, petroleum pitch, as well as special carbonaceous resins, polyols, pitch-hloov phenolic resins, synthetic resins, etc. Cov binders siv tau muab faib ua hom hauv qab no:

Pitch- raws li cov ntaub ntawv. Coal tar pitch yog cov khoom siv thermoplastic nrog qhov zoo xws li muaj zog affinity nrog graphite thiab magnesia, siab residual carbon nqi tom qab carbonization, thiab tus nqi qis; nws tau dav siv yav dhau los. Txawm li cas los xij, thee tar pitch muaj carcinogenic aromatic hydrocarbons, tshwj xeeb tshaj yog qib siab ntawm benzopyrene. Vim muaj kev paub txog ib puag ncig, kev siv cov thee tar pitch tam sim no txo ​​qis.

Resin- cov ntaub ntawv raws li. Synthetic resin yog tsim los ntawm cov tshuaj tiv thaiv ntawm phenol thiab formaldehyde. Nws tuaj yeem sib xyaw zoo nrog cov khoom siv refractory nyob rau hauv chav tsev kub thiab muaj cov pa roj carbon residual siab tom qab carbonization, ua rau nws lub ntsiab binder tam sim no siv rau MgO-C cib. Txawm li cas los xij, cov qauv hauv cov iav iav tsim tom qab nws cov carbonization tsis zoo rau cov thermal poob siab thiab oxidation tsis kam ntawm cov khoom siv refractory.

Hloov cov ntaub ntawv raws li suab thiab resin. Yog tias lub binder tuaj yeem tsim cov qauv 镶嵌 thiab hauv -situ carbon fibers tom qab carbonization, nws tuaj yeem txhim kho qhov siab - qhov kub thiab txias ntawm cov khoom siv refractory.

Antioxidants
Txhawm rau txhim kho oxidation tsis kam ntawm MgO-C cib, cov khoom siv me me feem ntau tau ntxiv. Cov tshuaj ntxiv muaj xws li Si, Al, Mg, Al-Si, Al-Mg, Al-Mg-Ca, Si-Mg-Ca, SiC, B₄C, BN, thiab tsis ntev los no tau tshaj tawm Al-B-C thiab Al{C1} {10}. Lub mechanism ntawm additives yuav roughly faib ua ob yam: ib tug yog los ntawm ib tug thermodynamic foundations, qhov twg nyob rau hauv lub kub ua hauj lwm, cov additives los yog lawv cov tshuaj tiv thaiv cov khoom nrog carbon muaj ib tug ntau affinity rau oxygen dua cov pa roj carbon, yog li nws nyiam oxidized thiab tiv thaiv cov pa roj carbon; Lwm qhov yog los ntawm qhov kev xav kinetic, qhov twg cov khoom sib txuas tsim los ntawm cov khoom siv ntxiv ua haujlwm nrog O₂, CO, lossis carbon hloov cov microstructure ntawm cov pa roj carbon- muaj cov khoom siv refractory, xws li nce ntom, thaiv qhov hws, thiab cuam tshuam cov diffusion ntawm oxygen thiab cov khoom siv tshuaj tiv thaiv.