Alumina Carbon Plug Qws

Alumina Carbon Plug Qws

Lub luag haujlwm tseem ceeb ntawm Aluminium plug Qws yog los tswj hwm tus nqi txaus ntawm Molten Steel nyob rau hauv lub intermediate ladle. Tshuab Argon lossis lwm yam khoom siv inert rau hauv cov av sib txuas yuav pab tswj hwm thiab huv cov pas dej Molten Lub cev ntawm tus pas nrig yog tsuas yog siv tau ntawm Al-C pawg, thaum lub taub hau yog tsuas yog tsim ntawm C + LIC, C + MGO MGO, thiab C + ZRO2 Cheebtsam.
Xa kev nug
Tsham tam sim no
Hauj lwm lawm

Kev piav qhia ntawm Alumina Carbon ntsaws Qws

 

Alumina carbon ntsaws rod yog ib qho tseem ceeb ua khoom lag luam refractory hauv nraus lub tshuab ua haujlwm, muaj ib lub cev thiab pas nrig. Lub cev nqaj lub cev yog ua los ntawm corundum thiab graphite li cov ntaub ntawv raw, thiab lub taub hau rod yog ua los ntawm silicon carbide thiab zircon xuab zeb ua cov khoom raw. Txhawm rau ua kom tiav cov haujlwm ntawm kev tawm tsam ntawm oxidation, tsis kam mus rau Molten Steel yaig thiab corrosion ntawm cov khoom. Lub alumina carbon ntsaws pas nrig yog tsim los ntawm isostatic nias, qhuav, thiab raug rho tawm hauv qhov chaw tsis oxidizing.

 

Alumina carbon ntsaws rod muaj cov yam ntxwv ntawm cov yam ntxwv ntawm cov hlau yaig, Kuj rau cov hlau corrosion, thiab purification ntawm cov hlau. Lub luag haujlwm tseem ceeb yog qhib thiab kaw qhov nruab nrab ntawm kev sib tw, thiab tswj hwm tus nqi txaus ntawm Molten Steel los ntawm Intermediate ladle rau lub crystallizer. Nws tseem muaj peev xwm ua kom tawg argon lossis lwm yam roj inert mus rau hauv pob nruab nrab ntawm cov argon tshuab lub qhov ntsaws.

 

Qhov saum npoo ntawm lub stopper yog coated nrog anti oxidation khoom. Hauv qab no 1000 degree, lub ntsej muag zoo nkauj ci tau tsim nyob rau saum npoo, nrog muaj zog adhesion thiab txhim kho kev ua kom muaj zog antioxidant.

 

Yam

Rod lub cev

Rod Taub Hau

AL2O3 (%)

Ntau dua los yog sib npaug rau 55

 

C + SIC (%)

Ntau dua los yog sib npaug rau 25

Ntau dua los yog sib npaug rau 15

ZO2 (%)

 

Ntau dua los yog sib npaug rau 70

Porosity (%)

Tsawg dua los yog sib npaug rau 20

Tsawg dua los yog sib npaug rau 20

Txias Crushing lub zog (mpa)

Ntau dua los yog sib npaug rau 20

Ntau dua los yog sib npaug rau 22

Modulus ntawm kev sib nqus (MPA)

Ntau dua los yog sib npaug rau 5

Ntau dua los yog sib npaug rau 7

Ntom ntom (g \/ cm³)

Ntau dua los yog sib npaug rau 2.5

Ntau dua los yog sib npaug rau 2.65

Thermal poob siab tsis kam

(sij hawm)

>5

>5

 

Yam ntxwv tseem ceeb

1) anti oxidation, anti steel corrosion

2) Purification ntawm Molten Steel

3) Tswj tus nqi txaus ntawm Molten Steel los ntawm Intermediate ladle rau lub crystallizer.

 

Lub hom phiaj tseem ceeb

Lub luag haujlwm tseem ceeb ntawm alumina carbon ntsaws rod yog qhib thiab tswj hwm tus nqi sib npaug ntawm Molten Steel los ntawm lub Intermediate ladle rau lub crystallizer.

 

Koj puas xav nrhiav tus kws xa khoom ntawmAlumina Carbon Plug Qws?

Koj puas xav nrhiav ib tus neeg xa khoom ruaj khov thiab muaj peev xwm?

Tom qab ntawv thov hu rau peb.

 

Hu rau kuv:

Email: {{{{{1}\/sdwenping@163.com

Tel: {{{86-0533-4188518 \/ fev: 86-0533-4188518

Rose: {+86-13275332819 (WeChat \/ Whatsapp Tus lej)

Cim npe nrov: Alumina carbon ntsaws cov pas nrig, Suav teb, manufacturers, cov chaw muag khoom, Hoobkas, siv, cov cuab yeej

Xa kev nug
Tiv tauj peb
  • Tel: +86-533-4188518
  • Mob: +8613275332819
  • E - Xa Ntawv: sdwenping@163.com
  • Ntxiv: PAV 711, No.3, Yanhe Txoj kev, Boshan, Zibo, Shandong, Phiaj suav

(0/10)

clearall